| 用铬传感器测定碳饱和铁液中Cr的活度 |
| 徐秀光;王常珍;于化龙;曲向东 |
| 东北大学;沈阳;110006;东北大学;沈阳;110006;东北大学;沈阳;110006;东北大学;沈阳;110006 |
|
| [Cr]Fe |
| No Author |
引用本文:
徐秀光;王常珍;于化龙;曲向东. 用铬传感器测定碳饱和铁液中Cr的活度[J]. 金属学报, 1997, 33(9): 959-963.
,
,
,
.
[Cr]Fe[J]. Acta Metall Sin, 1997, 33(9): 959-963.
1Iwase M.Scand J Metall,1988;17:50 2岩崎克博,斋藤典生,妹尾弘已,长家利男雀部实.日本金属学会会报,1988;27:474 3黄艳玲,张千象,洪彦若.北京矿冶研究总院学报,1994;3:67 4Goto K S,Sasabe M,Iguchi Y,Iwase M,Onou-ye T.Solid State Ionics,1990;40/41:770 5Inouye T K,Fujiware H,Iwase M.Metall Trans,1991;22B:475 6Hoshino H,Shimada T,yamamoto M,Iwase M Metall Transt 1992;23B:169 7Toker N Y,Darxen L S,Muan A.Metall Trans.1991;22B:225_ |
|