| 形变奥氏体连续冷却相变后α晶粒尺寸的预测 |
| 刘振宇;王国栋;张强 |
| 东北大学轧制技术与连轧自动化国家重点实验室;东北大学压力加工系 |
|
| GRAIN SIZE PREDICTION AFTER CONTINUOUSLY COOLING TRANSFORMATION FROM DEFORMED AUSTENITE TO FERRITE |
| LIU Zhenyu; WANG Guodong;(Department of Metal Forming; Northeastem University; Shenyang 110006) ZHANG Qiang (State Key Laboratory of RollingTechnology and Tandem Rolling Automation; Northeastern University; Shenyang110006) |
引用本文:
刘振宇;王国栋;张强. 形变奥氏体连续冷却相变后α晶粒尺寸的预测[J]. 金属学报, 1995, 31(22): 468-172.
,
,
.
GRAIN SIZE PREDICTION AFTER CONTINUOUSLY COOLING TRANSFORMATION FROM DEFORMED AUSTENITE TO FERRITE[J]. Acta Metall Sin, 1995, 31(22): 468-172.
| 1UmemotoM.ActaMetall,1986;34:13772CahnJW.ActaMetall,1956;4:5723TamuraI,SekineH,TanakaT,OuchiC.ThermomechanicalProcessingofHighStrengthLowAlloySteels,ButterworthsPublicationHouse,19884刘振宇,王国栋,张强.钢铁研究学报,1994;6:315矢田浩.塑性加工,1987;28:4136刘振宇,王国栋,张强,马龙翔.金属学报,1994;30:B2777KerkaldyJS.ScandJMetall,1991;20:508LiuZ,WangW,WangG,ZhangQ.JMaterSciTechnol,1993;9:215 |
|