金属学报  1994, Vol. 30 Issue (11): 481-490    
  论文 本期目录 | 过刊浏览 |
贝氏体相变理论新进展及学术分歧
方鸿生;王家军
清华大学
AN OVERVIEW OF RECENT PROCESSES AND ARGUMENTS ON BAINITIC TRANSFORMATION THEORY
FANG Hongsheng;WANG Jiajun (Tsinghua University; Beijing)(Manuscript received 25 March; 1994)
引用本文:

方鸿生;王家军. 贝氏体相变理论新进展及学术分歧[J]. 金属学报, 1994, 30(11): 481-490.
, . AN OVERVIEW OF RECENT PROCESSES AND ARGUMENTS ON BAINITIC TRANSFORMATION THEORY[J]. Acta Metall Sin, 1994, 30(11): 481-490.

全文: PDF(897 KB)  
摘要: 介绍了贝氏体相变领域切变和扩散控制台阶长大理论的核心内容;论述了贝氏体相变理论领域的主要研究成果及争论焦点:涉及贝氏体定义、转变不完全性、溶质拖曳及类拖曳效应、表面浮突的形态、特征及本质、相变产物的晶体学、贝氏体铁素体初始碳含量、贝氏体“中脊”、下贝氏体碳化物来源及形成模型等.
关键词 : 贝氏体,  扩散控制台阶长大机制,  切变机制    
Abstract:The main points of view about shear and difusion for the bainitic transformation, which include some important research results and key controversial points,i.e., bainite definition, incomplete phenomenon, solute-drag and solute drag-like effects,the shape, characteristics,nature of the surface relief,crystallography,initial carbon content in bainitic ferrite, the so-called midrib of bainite, source and formation model of lower bainitic carbide,etc., were briefly reviewed.Correspondent: WANG Jiajun, Department of Materials Science and Engineering,(Tsinghua University,Beijing 100084)
Key words: bainite    diffusion-controlled ledgewise growth mechanism    shearism
收稿日期: 1994-11-18     
基金资助:国家自然科学基金
1RobertsonJM.JISI,1929;119:3912 DavenportES,BainEC.TransAIME,1930;90:1173方鸿生,王家军.金属热处理学报,1994;15(4):待发表4 Ko T,CottrellSA.JISI,1952;172:3075 KoT.JISI,1953;175:166ChristianJW.DecompositionAustenitebyDiffusionalProcesses.NY:IntersciencePublishers,1962:3717OblackJM,HehemannRF.Transformations&HardenabilityinSteels,AnnArbor,MI:ClimaxMolybdenumCompany,1967:158HehemannRF,TrioanoAR.MetProg,1956;70(2):979HehemannRF.In:AaronsonHIed.,PhaseTransformations.MetalsPark,OH:ASM,1970:39710BhadeshiaHKDH,EdmondsDV.Metall Trans,1979:10A:89511康沫狂.西北工业大学学报,1990;增刊:112俞德刚.合金中温相变学说的发展及其分歧,上海交通大学科技交流室,198913冯华,康沫狂,李春信.第一届全国贝氏体相变会议论文集,1987,广东,惠州14BhadeshiaHKDH,EdmondsDV.ActaMetall,1980;28:126515EntiwRI.In:ZackayVF.AaronsonHIeds.,DecompositionofAustenitebyDiffusionProcesses.NY:Intersciencepublishers,1962:29516HillertM.In:ZackayVF,AaronsonHIeds.,DecompositionofAustenitebyDiffusionalProcesses.IntersciencePublishers,NY:IntersciencePublishers,1962:19717俞德刚,陈大军,郑经弘.贝氏体铁素体的相变基元和贝氏体θ碳化物的来源及相变的表面浮雕,上海交通大学材料系,1988:418AaronsonHI.In:ZackayVF,AaronsonH I,eds.,DecompositionofAustenitebyDiffusionalPro-cesses,NY:IntersciencePublishers,1962:38719RigsbeeJM,AaronsonHI.ActaMetall,1979;27:35120徐启昆,康戈文.重庆大学学报,1993;16(3):5921方鸿生,王家军.兵器材料科学与工程,1994;17(2):322HuangD,ThomasG.MetallTrans,1972;3A:34323PickeringFB.MetallTrans,1977;8A:10924KaufmanL,RacliffeL,CohenM.In:ZackayVF,AaronsonHLeds.,DecompositionofAustenitebyDiffusionalProcesses.NY:IntersciencePublishers,1962:31325杨柳.清华大学博士学位论文,198826 PurdyGR,HillertM.ActaMetall.1984,32:82327 Hehemann R F,Kinsman K R,AaronsonHI.MetallTrans,1972;3A:107728RigsbeeJM,MennonE SK,LeeHJ,AaronsonHI.ScrMetall,1983;17:146129 BhadeshiaHKDH,ScrMetall,1983;17:147530 BhadeshiaHKDH.ScrMetall.1987;21:101731BhadeshiaHKDH.ChristianJW.MetallTransA,1990;21A:76732AaronsonHI,ReynoldsWT.Jr,ShifletGJ,SpanosG.MetallTrans,1990;21A:134333 ShifletGJ,AaronsonHI.MetallTrans,199o;21A:141334 ReynoldsWT.Jr,LiFZ,ChuiCK,ArronsonHI,MetallTrans,1990;21A:143335LeeHJ,SpanosG,ShifletGJ,AaronsonHI.ActaMetall,1988;36:112936AaronsonHI.TheMechanismofPhaseTransformationsinCrystallineSolids.London:InstituteofMetals,1969;27037康沫狂,胡光立,谭若兵.西北工业大学学报,1990;增刊:3438 WechslerMS,LiebermanDS,ReadTA.Trans AIME,1953;194:150339BowlesJS,MackenieJK.ActaMetall,1954;2:12940BilbyBA,ChristianJW.TheMechanismof PhaseTransformationsinMetals.London:InstituteofMetals,1956:12141 CornelisI,WaymanCM.ActaMetall,1974;22:30142 SmithS,BowlesJS.ActaMetall,1960;8:40543GoldensteinH,AaronsonHI.MetallTrans,1990;21A:146544WeverF,MathieuK,MittKW.InstEnsenforsch,1940;22:945LymanT,TroianoAR.Trans ASM,1946;37:40246BoswellPG,KinsmanKR,ShifletGJ,AaronsonHI.MechanicalPropertiesandPhaseTransfor-mationsinEngineeringMaterials.Warrendale,PA:TSM-AIME,1986:44547AaronsonHI.In:AaronsonHIed.,PhaseTransformations.MetalsPark,OH:ASM,1970:31348ReynoldsWT.Jr,Brenner SS,ArronsonHI.ScrTrans.,1988;22:134349杨柳,方鸿生,孟至和.金属学报,1992;28:A1650ReynoldsWT.Jr,LiuSK,LiFZ,HartfieldS,ArronsonHI.MetallTrans,1990,21A:147951BradleyJR,AaronsonHI.MetallTrans,1981,12:172952LiuSK,ReynoldsWTReynoldsJr,HuH,ShifletGJ,AaronsonHI.MetallTrans,1985;16A:45753ClarkHM,WaymanCM.PhaseTransformations.MetalsPark,OH:ASM,1970:5954AaronsonHI.ScrMetall,1980;14:82555LeeHJ,AaronsonHI.AclaMetall,1988;36:78756DahmenU.ScrMetall,1987,21:102757BhadeshiaHKDH.ScrMetall,1980;14:82158 BhadeshiaHKDH.ActaMetall,1981;29:111759ChristianJW,EdmondsDV.ProcInterConfonPhaseTransformationsinFerrousAlloys,Warrendale,PA:TSM-AIME,1983:29360LairdC,Aaronson,HI.ActaMetall,1967;15:7361LiuYC,AaronsonHI.ActaMetall,1970;18:84562KinsmanKR,EichenE,AaronsonHI.MetallTrans.1975;6A:30363 PitschW.ArchEisenhuettenw,1963;34,38164PickeringFB.Transformation&Hardenabilityinsteels.AnnArbor,MI:ClimaxMolybdenumCompany,1967:10965BhadeshiaHKDH.ActaMetall,1980;28:110366ShackletonDN,KellyPM.PhysicalPropertiesofMartensite&Bainite,Specialreport,ISI,1965;93:12667WellsMGH.ActaMetall,1964;12:38968AaronsonHI,PlichtaMR,FrantiGW,RussellKC.MetallTrans,1978;9A:36369OkaM,OkamotoH,IshidaK.MetallTrans,1990;21A:84570SrinivasanGR,WaymanCM.ActaMetall,1968;16:60971SandvikBPJ,WaymanCM.MetallTrans,1983;14A:82372AaronsonH I,LeeHJ.ScrMetall,1987;21:101173BhadeshiaHKDH,WaughAR.ActaMetall,1982;30:77574KinsmanKR,EichenE,AaronsonHI.MetallTrans,1971;2A(1):34675刘文西,邹美运,马福本,金属学报,1982;17:13776GreningerAB,TroianoAR.TransAIME,1940;140:30777 SchaaberO.TransAIME,1955;203:55978KennonNF,EdwardsRH.J AustInst.Metals,1970;15:19579OkamotoH,OkaM.MetallTrans,1985;16A:225780OkamotoH.MetallTrans,1986;17A:111381BilbyBA,ChristianJW.JISI,1961;197:12282GreningerAB,TroianoAR.TransAIME,1949;185:59183徐祖耀.马氏体相变与马氏体,北京:科学出版社,1980:10784WasilewskiRJ.MetallTrans,1970;1A:264185SpanosG,FangHS,SarmaDS,AaronsonHI.MetallTrans,1990;21A:139186LaiGY.MetallTrans,1975;6A:146987FangHS,WangJJ,ZhengYK.MetallTrans,1994;25(9),inpublishing88JinQ,FangHS.MetallTrans,1990;21A:263789王家军,清华大学博士学位论文,199390HoneycombeRWK,In:MarderAR,GoldsteinJIeds.,ProceedingofanInternationalConferenceonPhaseTransformationsinFerrousAlloys,Warrendale,PA:TSM-AIME,1983;25991方鸿生,王家军.金属学报,1994;30:491l
[1] 赵亚峰, 刘苏杰, 陈云, 马会, 马广财, 郭翼. 铁素体-贝氏体双相钢韧性断裂过程中的夹杂物临界尺寸及孔洞生长[J]. 金属学报, 2023, 59(5): 611-622.
[2] 朱彬, 杨兰, 刘勇, 张宜生. 基于纳米压痕逆算法的热冲压马氏体/贝氏体双相组织的微观力学性能[J]. 金属学报, 2022, 58(2): 155-164.
[3] 朱东明, 何江里, 史根豪, 王青峰. 热输入对Q500qE钢模拟CGHAZ微观组织和冲击韧性的影响[J]. 金属学报, 2022, 58(12): 1581-1588.
[4] 蒋中华, 杜军毅, 王培, 郑建能, 李殿中, 李依依. M-A岛高温回火转变产物对核电SA508-3钢冲击韧性影响机制[J]. 金属学报, 2021, 57(7): 891-902.
[5] 刘曼, 胡海江, 田俊羽, 徐光. 变形对超高强贝氏体钢组织和力学性能的影响[J]. 金属学报, 2021, 57(6): 749-756.
[6] 彭云,宋亮,赵琳,马成勇,赵海燕,田志凌. 先进钢铁材料焊接性研究进展[J]. 金属学报, 2020, 56(4): 601-618.
[7] 王占花, 惠卫军, 谢志奇, 张永健, 赵晓丽. 回火对钒钛微合金化Mn-Cr系贝氏体型非调质钢组织和性能的影响[J]. 金属学报, 2020, 56(11): 1441-1451.
[8] 田亚强,田耕,郑小平,陈连生,徐勇,张士宏. 淬火配分贝氏体钢不同位置残余奥氏体C、Mn元素表征及其稳定性[J]. 金属学报, 2019, 55(3): 332-340.
[9] 万响亮, 胡锋, 成林, 黄刚, 张国宏, 吴开明. 两步贝氏体转变对中碳微纳结构钢韧性的影响[J]. 金属学报, 2019, 55(12): 1503-1511.
[10] 徐士新, 余伟, 李舒笳, 王坤, 孙齐松. 预变形温度对纳米贝氏体相变动力学及组织的影响[J]. 金属学报, 2018, 54(8): 1113-1121.
[11] 武慧东, 宫本吾郎, 杨志刚, 张弛, 陈浩, 古原忠. Fe-1.5(3.0)%Si-0.4%C合金贝氏体不完全转变现象及伴随的渗碳体析出[J]. 金属学报, 2018, 54(3): 367-376.
[12] 胡小锋, 姜海昌, 赵明久, 闫德胜, 陆善平, 戎利建. 一种Fe-Cr-Ni-Mo高强高韧合金钢焊接接头的组织和力学性能[J]. 金属学报, 2018, 54(1): 1-10.
[13] 陈连生, 李跃, 张明山, 田亚强, 郑小平, 徐勇, 张士宏. 两相区位错增殖对Mn元素配分及低碳钢贝氏体组织的影响[J]. 金属学报, 2017, 53(11): 1418-1426.
[14] 桂晓露,张宝祥,高古辉,赵平,白秉哲,翁宇庆. Q-P-T处理贝氏体/马氏体复相高强钢疲劳断裂特性研究*[J]. 金属学报, 2016, 52(9): 1036-1044.
[15] 崔君军,陈礼清,李海智,佟伟平. 等温淬火低合金贝氏体球墨铸铁的回火组织与力学性能*[J]. 金属学报, 2016, 52(7): 778-786.