| NdFeB永磁材料氧化行为的研究 |
| 华宏慈;王葛亚;徐庆镇;金慧娟;许桂琴 |
| 中国科学院上海冶金研究所;上海(200050);中国科学院上海冶金研究所;中国科学院上海冶金研究所;上海钢铁研究所;上海钢铁研究所 |
|
| OXIDATION OF NdFeB PERMANENT MAGNETS IN HUMID ATMOSPHERE |
| HUA Hongci;WANG Geya Shanghai Institute of Metallurgy; Academia Sinica; XU Qingzhen;JIN Huijuan;XU Guiqin Shanghai Iron and Steel Research Institute |
引用本文:
华宏慈;王葛亚;徐庆镇;金慧娟;许桂琴. NdFeB永磁材料氧化行为的研究[J]. 金属学报, 1991, 27(1): 141-144.
,
,
,
,
.
OXIDATION OF NdFeB PERMANENT MAGNETS IN HUMID ATMOSPHERE[J]. Acta Metall Sin, 1991, 27(1): 141-144.
1 Sagawa M, Fujimura S, Togawa N et al. J Appl Phys. 1984; 55: 2083 2 Croat J J, Herbst J F, Lee R W et al. J Appl Phys, 1984; 55: 2078 3 Sagawa M Hirosawa S, Yamamoto H et al. Jpn J Appl Phys, 1987; 26: 785 4 Jacobson J. Kim A. J Appl Phys, 1987; 61: 3763 5 Willman C J, Narasimhan K S V L. J Appl Phys, 1987; 61: 3766 6 Nakamura H, Pukuno A, Yoneyama T. In: Proc 10th Int Workshop Rare Earth Magnets and Their Applications, Tokyo, 19 May, 1989, Tokyo, 1989; 315 7 Hasebe A, Otsuki E. In; Proc 10th Int Workshop Rare Earth Magnets and Their Applications, Tokyo, 1989: 383 8 Sagawa M. Fujimura S, Yamamoto H et al. In: Strnat. K J ed. Proc 8th Int Workshop on Rare Earth Magnets and Their Applications and the 4th Int Symp on Magnetic Anisotropy and Coercivity in Rare Earth-Transition Metal Alloys, Dayton, Ohio: Univ of Dayton. 1985: 587 9 Boller H, Oesterreicher H. J Less-Common Met, 1984; 103: L5 10 Herbst J F. Croat J J. Pinkerton F E et al. Phys Rev, 1984; B29: 4176 11 Qian Xiangrong, Jin Huijuan, Xu Ouiqing, et al. In: Strnat K J ed. Proc 8th Int Workshop on Rare Earth Magnets and Their Applicattons and the 4th Int Symp on Magnetic Anisotropy and Coercivity in Rare Earth-Transition Metal Alloys, Dayton. Ohio: Univ of Dayton. 1985: 693 12 Pan S. In: 5th International Symposium on magnetic anisotropy and Coercivity in Rare Earth-Trasiotion metal alloys, September 3, 1987, Bad Soden. FRG, 1987: 419 13 Bate G. In: Wohlfarth E P ed. Ferromagnetic Materials: A Handbook on the Properties of Magn etically Ordered Substances, Vol.II, Amsterdam: North-Holland. 1980: 381 14 华宏慈.钕铁硼永磁材料氧化行为及防护(内部报告).19901 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|