| 钢轨显微组织与疲劳性能 |
| 周清跃;周晨光 |
| 工程师;北京(100081);铁道部科学研究院金属及化学研究所;铁道部科学研究院 |
|
| MICROSTRUCTURE AND FATIGUE PROPERTIES OF RAIL STEELS |
| ZHOU Qingyue;ZHOU Chenguang (China Academy of Railway Sciences; Beijing Engineer;Metal and Chemistry Research Institute;China Academy of Railway Sciences;Beijing 100081 |
引用本文:
周清跃;周晨光. 钢轨显微组织与疲劳性能[J]. 金属学报, 1990, 26(4): 73-78.
,
.
MICROSTRUCTURE AND FATIGUE PROPERTIES OF RAIL STEELS[J]. Acta Metall Sin, 1990, 26(4): 73-78.
1 周清跃.铁道部科学研究院硕士论文,1986 2 Gan D, Weertman J. Eng Fract Mech, 1981; 15; 87 3 Gray G T III, Thompson A W, Williams, J. C. Metall Trans, 1985; 16A: 753 4 Bouse G K, Bernstein I M, Stone D H, ASTM STP 644, 1978: 145--166 5 周晨光,周镇国,邵扬道.铁道学报,1985;7(1) :99S |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|