| 5CrMnMo钢的热疲劳裂纹研究 |
| 何世禹;李瑛;刘剑虹 |
| 副教授;哈尔滨(150006);哈尔滨工业大学金属学教研室;哈尔滨工业大学;哈尔滨工业大学 |
|
| THERMAL FATIGUE CRACK IN 5CrMnMo STEEL |
| HE Shiyu;LI Ying;LIU Jianhong Harbin Institute of Technology Faculty of Metal;Harbin Institute of Technology; Harbin |
引用本文:
何世禹;李瑛;刘剑虹. 5CrMnMo钢的热疲劳裂纹研究[J]. 金属学报, 1990, 26(4): 62-65.
,
,
.
THERMAL FATIGUE CRACK IN 5CrMnMo STEEL[J]. Acta Metall Sin, 1990, 26(4): 62-65.
1 平修二.热应力热疲劳,东京:日刊工业新闻社,1974:6 2 Malm S. Norstroem L-A. Met Sci, 1979; 13: 545 3 Young R M, Moore A A, Gibbons C L II. Ind Heat, 1981; 48(7) : 24 4 Yamada Y, Yoshimura N, Sakurai T. Int J Mech Sci, 1968; 10: 343 5 张静华,唐亚俊,于洋,张济山,胡壮麒.金属学报,1988;24:A254 6 Coffin L F Jr. Trans ASME, 1954; 76: 931L |
|