| 灰铸铁激光处理层内的残余奥氏体及应变诱发马氏体 |
| 李成劳;沈莲 |
| 西安交通大学材料工程系;讲师;西安(710049);西安交通大学 |
|
| RESIDUAL AUSTENITE AND STRAIN-INDUCED MARTENSITE IN LASER HARDENING LAYER ON GRAY CAST IRON |
| LI Chenglao;SHEN Lian Xi'an Jiaotong University Li Chenglao; Department of Material Engineering; Xi'an Jiaotong University;Xi'an 710049 |
引用本文:
李成劳;沈莲. 灰铸铁激光处理层内的残余奥氏体及应变诱发马氏体[J]. 金属学报, 1989, 25(6): 74-77.
,
.
RESIDUAL AUSTENITE AND STRAIN-INDUCED MARTENSITE IN LASER HARDENING LAYER ON GRAY CAST IRON[J]. Acta Metall Sin, 1989, 25(6): 74-77.
1 Belfote D. In: Ready J E ed, Lasers in Modern Industry, Dearborn MI: Society of Manufacturing Engineers, 1979: 128 2 Chen C H, Altstetter C J, Rigsbee J M. Metall Trans, 1984; 15A: 719 3 Dash S, Brown N. Acta Metall, 1966; 14: 595 4 徐祖耀.马氏体相变与马氏体,北京:科学出版社,1980:421 5 Maxwell P C, Goldberg A, Shyne J C. Metall Trans, 1974; 5: 1319$ |
|