| Cu-Zr和Cu-Zr-Si的时效析出特性及冷变形对时效析出的影响 |
| 董志力;唐祥云;堀茂德;藤谷涉 |
| 清华大学;清华大学;大阪大学工学部;大阪大学工学部 |
|
| AGING PRECIPITATION OF Cu-Zr AND Cu-Zr-Si ALLOYS AND AFFECTED BY COLD WORKING |
| DONG Zhili;TANG Xiangyun;HORI Shigenori;FUJITANI Wataru Qinghua University; Beijing Faculty of Engineering; Osaka University DONG Zhili; Department of Material Science and Engineering; Qinghua University;Beijing 100084 |
引用本文:
董志力;唐祥云;堀茂德;藤谷涉. Cu-Zr和Cu-Zr-Si的时效析出特性及冷变形对时效析出的影响[J]. 金属学报, 1989, 25(6): 78-81.
,
,
,
.
AGING PRECIPITATION OF Cu-Zr AND Cu-Zr-Si ALLOYS AND AFFECTED BY COLD WORKING[J]. Acta Metall Sin, 1989, 25(6): 78-81.
1 小林正男,岩村卓郎,大坪正明,泉田益弘.日本金属学会会报,1988;27:284 2 陶志刚,仪表材料,1986;17:135 3 坂本光雄,日本金属学会会报,1985;24:494 4 Sarin V K, Grant N J. Powder Metall Int, 1979; 11: 153 5 铃木寿,川胜一郎,北野均,村赖昭次.日本金属学会志,1967;31:14 6 铃木寿,菅野幹宏,川胜一郎,日本金属学会志,1969;33:628k |
|