| 18Ni合金在弹性应力作用下再结晶诱发塑性现象 |
| 尹钟大;周永康 |
| 哈尔滨工业大学金属材料热处理教研室;副教授;哈尔滨(150006);上海离心机械研究所 |
|
| RECRYSTALLIZATION-INDUCED PLASTICITY PHENOMENON IN 18Ni MARAGING STEEL UNDER ELASTIC STRESS |
| YIN Zhongda;ZHOU Yongkang Harbin Institute of Technology Shanghai Centrifugal Machinery Research Institute YIN Zhongda; Pacxlty of Heat Treatment of Materials Harbin Institute of Technology; 150006 Harbin |
引用本文:
尹钟大;周永康. 18Ni合金在弹性应力作用下再结晶诱发塑性现象[J]. 金属学报, 1989, 25(5): 54-58.
,
.
RECRYSTALLIZATION-INDUCED PLASTICITY PHENOMENON IN 18Ni MARAGING STEEL UNDER ELASTIC STRESS[J]. Acta Metall Sin, 1989, 25(5): 54-58.
1 周永康.哈尔滨工业大学硕士学位论文,1988 2 胡郇.国外金属材料,1983;(1) :54 3 牧正志,田村今男.材料,1981;30(329) :211 4 Li J E M. J Appl Phys, 1962; 33: 2958 5 Bailey J E. Philos Mag, 1960; 5: 83 |
|