| Mo-La合金丝的表面偏析研究 |
| 胡德清;张兆祥;赵兴钰 |
| 北京大学;北京大学无线电电子学系;副教授;北京(100871);北京大学 |
|
| SURFACE SEGREGATION IN Mo-La ALLOY WIRE |
| HU Deqing;ZHANG Zhaoxiang;ZHAO Xingyu Peking University; Beijing ZHANG Zhaoxiang; Department of Radio Electronics; Peking University; 100871 Beijing |
引用本文:
胡德清;张兆祥;赵兴钰. Mo-La合金丝的表面偏析研究[J]. 金属学报, 1989, 25(5): 133-138.
,
,
.
SURFACE SEGREGATION IN Mo-La ALLOY WIRE[J]. Acta Metall Sin, 1989, 25(5): 133-138.
1 Ponec V. Catal Rev Sci Eng, 1975; 11: 41 2 Seah M P. Surf Sci, 1975; 53: 168 3 Goedel D M, Forrester A T, Johnson S. Rev Sci Instrum, 1980; 51: 1468 4 Buxbaum C. US Pat, 4 274 939, 1981 5 Davis L E, MacDonald N C, Palmberg P W, Riach G E, Weber R F. Handbook of Auger Flectron Spectroscopy, 2nd ed., Minnesota: Physical Eletronics Industries, 1976: 177 6 Miedema A R. Philips Tech Rev, 1975; 33: 149 7 Miedema A R. Philips Tech Rev, 1976; 36: 217 8 胡德清.北京大学硕士学位论文,1988 9 Lea C, Seah M P. Philips Mag, 1977; 35: 213 10 Zhang Zhaoxiang (张兆祥), Jiao Jintang (焦锦堂), Hu Deqing (胡德清). Proc 34th Int Field Emission Symp., Paris: les editions de physique, 1987: C6--283 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|