C对单晶高温合金持久性能的影响* |
余竹焕1( ), 刘林2 |
1 西安科技大学材料科学与工程学院, 西安 710054 2 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
EFFECT OF C ON THE RUPTURE PROPERTIES OF SINGLE CRYSTAL SUPERALLOYS |
YU Zhuhuan1( ), LIU Lin2 |
1 Department of Materials Science and Engineering, Xi′an University of Science and Technology, Xi′an 710054 2 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi′an 710072 |
引用本文:
余竹焕, 刘林. C对单晶高温合金持久性能的影响*[J]. 金属学报, 2014, 50(7): 854-862.
Zhuhuan YU,
Lin LIU.
EFFECT OF C ON THE RUPTURE PROPERTIES OF SINGLE CRYSTAL SUPERALLOYS[J]. Acta Metall Sin, 2014, 50(7): 854-862.
[1] |
Guo J T. Acta Metall Sin, 2010; 46: 513
|
[1] |
(郭建亭. 金属学报, 2010; 46: 513)
|
[2] |
Pollock T M, Murphy W H, Goldman W H, Antolokch S D, Stusrud R W, MacKay R A. Superalloys 1992, Warrendale: TMS, 1992: 125
|
[3] |
Liu G, Liu L, Zhang S X, Yang C B, Zhang J, Fu H Z. Acta Metall Sin, 2012; 48: 845
|
[3] |
(刘 刚, 刘 林, 张盛霞, 杨初斌, 张 军, 傅恒志. 金属学报, 2012; 48: 845)
|
[4] |
Wilson B C, Cutler E R, Fuchs G E. Mater Sci Eng, 2008; A479: 356
|
[5] |
Zhang Z, Lou L. J Mater Sci Technol, 2007; 23: 289
|
[6] |
Liu L, Huang T W, Zhang J, Fu H Z. Mater Lett, 2007; 61: 227
|
[7] |
Al-Jarba K A, Fuchs G E. JOM, 2004; (9): 50
|
[8] |
Tin S, Pollock T M, King W T. Superalloys 2000, Boston: TMS, 2000: 201
|
[9] |
Wasson A J, Fuchs G E. Mater Charact, 2012; 74: 11
|
[10] |
Tin S, Pollock T M. Mater Sci Eng, 2003; A348: 111
|
[11] |
Al-Jarba K A, Fuchs G E. Mater Sci Eng, 2004; A373: 255
|
[12] |
Liu L R, Jin T, Zhao N R, Wang Z H, Sun X F, Guan H R, Hu Z Q. Mater Lett, 2004; 58: 2290
|
[13] |
Cutler E R, Wasson A J, Fuchs G E. Scr Mater, 2008; 58: 146
|
[14] |
Liu L R, Jin T, Zhao N R, Sun X F, Guan H R, Hu Z Q. Mater Sci Eng, 2003; A361: 191
|
[15] |
Liu L R, Jin T, Zhao N R, Wang Z H, Sun X F, Guan H R, Hu Z Q. Mater Sci Eng, 2004; A385: 105
|
[16] |
Yu J J, Sun X F, Zhao N R, Jin T, Guan H R, Hu Z Q. Trans Nonferrous Met Soc China, 2006; 16: 1973
|
[17] |
Xiao L, Chen D L, Chaturvedi M C. Mater Sci Eng, 2006; A437: 157
|
[18] |
Zhou Y Z, Volek A. Mater Sci Eng, 2008; A479: 324
|
[19] |
Glas R, Jouiad M, Caron P. Acta Mater, 1996; 44: 4917
|
[20] |
Kamaraj M. Sadhana, 2003; 28: 115
|
[21] |
Raffaitin A, Monceau D, Andrieu E. Acta Mater, 2006; 54: 4473
|
[22] |
Kim I S, Cho B G, Seo S M. Mater Lett, 2008; 62: 1110
|
[23] |
Yu Z H. PhD Dissertation, Northwestern Polytechnical University, Xi′an, 2011
|
[23] |
(余竹焕. 西北工业大学博士学位论文, 西安, 2011)
|
[24] |
Yu Z H, Liu L, Zhao X B, Zhang W G, Zhang J, Fu H Z. China Foundry, 2010; 7: 352
|
[25] |
Qin X Z, Guo J T, Yuan C, Hou J S, Ye H Q. Mater Lett, 2008; 62: 258
|
[26] |
Wasson A J, Fuchs G E. Mater Charact, 2012; 74: 11
|
[27] |
Sun X T. Master Thesis, Shenyang University of Technology, 2007
|
[27] |
(孙新涛. 沈阳工业大学硕士学位论文, 2007)
|
[28] |
Wagner A, Shollock B A, Mclean M. Mater Sci Eng, 2004; A374: 270
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|