快淬Nd--Fe--B非晶厚带的晶化过程和非等温晶化动力学 |
王大鹏;包小倩;张茂才;朱洁 |
(北京科技大学新金属材料国家重点实验室; 北京 100083) |
|
CRYSTALLIZATION PROCESS AND NON–ISOTHERMAL CRYSTALLIZATION KINETICS OF MELT–SPUN Nd–Fe–B AMORPHOUS THICK RIBBONS |
WANG Dapeng; BAO Xiaoqian; ZHANG Maocai; ZHU Jie |
State Key Laboratory of Advanced Metals and Materials; University of Science and Technology Beijing; Beijing 100083 |
引用本文:
王大鹏 包小倩 张茂才 朱洁. 快淬Nd--Fe--B非晶厚带的晶化过程和非等温晶化动力学[J]. 金属学报, 2009, 45(2): 237-242.
,
,
,
.
CRYSTALLIZATION PROCESS AND NON–ISOTHERMAL CRYSTALLIZATION KINETICS OF MELT–SPUN Nd–Fe–B AMORPHOUS THICK RIBBONS[J]. Acta Metall Sin, 2009, 45(2): 237-242.
[1] Croat J J, Herbst J F, Lee R W, Pinkerton F E. J Appl Phys, 1984; 55: 2078
[2] Skomski R. J Appl Phys, 1994; 76: 7059
[3] Biswas K, Ram S, Schultz L, Eckert J. J Alloys Compd, 2005; 397: 104
[4] Li F S, Zhang T, Guan S K, Shen N F. Trans Nonferrous Met Soc China, 2004; 14: 840
[5] Guschl P C, Kim H S, Otaigbe J U. J Appl Polym Sci, 2001; 83: 1091
[6] Horiguchi T, Sekizawa H, Murata M, Kondo H, Kawagoe T, Iguchi Y, Kohn K, Mizoguchi T. Key Eng Mater, 1990; 40: 87
[7] Gao Y Q, Wang W. J Non–Cryst Solids, 1986; 81: 129
[8] Kempen A TW, Sommer F, Mittemeijer E J. J Mater Sci, 2002; 37: 1321
[9] Kissinger H E. Anal Chem, 1957; 29: 1702
[10] Lu K. Mater Sci Eng, 1996; R16: 161
[11] Trujillo M P, Orozco A, Casas–Ruiz M, Ligero R A, Jimenez–Garay R. Mater Lett, 1995; 24: 287
[12] Cahn J W. Acta Metall, 1956; 4: 572
[13] Yinnon H, Uhlmann D R. J Non–Cryst Solids, 1983; 54: 253
[14] Gao Y Q,WangW, Zheng F Q, Liu X. J Non–Cryst Solids, 1986; 81: 135
[15] Jain R, Saxena N S, Bhandari D, Sharma S K, Rao K V R. Phys B (Amsterdam, Neth), 2001; 301B: 341
[16] Liu X J, Hui X D, Chen G L. Mater Sci Forum, 2005; 475: 3385
[17] Soliman A A, Al–Heniti S, Al–Hajry A, Al–Assiri M, Al–Barakati G. Therm Acta, 2004; 413: 57
[18] Christian J W. Theory of Transformation in Metals and Alloys. 2nd ed., Oxford: Pergamon Press; 1975: 487
[19] Takeuchi A, Inoue A. Mater Trans, 2005; 46: 2817
[20] Wang Y H, Yang Y S. Amorphous Alloys. Beijing: Metallurgical Industry Press; 1989: 96
(王一禾, 杨膺善. 非晶态合金. 北京: 冶金工业出版社; 1989:96) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|