Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (8): 785-790    DOI:
Current Issue | Archive | Adv Search |
BHAVIOUR OF COMPLEX ELASTIC MODULUS AND INTERNAL FRICTION DURING EUTECTOID DECOMPOSITION
LIU Junmin; ZHANG Jinxiu (Zhongshan University; Guangzhou 510275)(Manuscript received 1995-08-09; in revised form 1996-04-11)
Cite this article: 

LIU Junmin; ZHANG Jinxiu (Zhongshan University; Guangzhou 510275)(Manuscript received 1995-08-09; in revised form 1996-04-11). BHAVIOUR OF COMPLEX ELASTIC MODULUS AND INTERNAL FRICTION DURING EUTECTOID DECOMPOSITION. Acta Metall Sin, 1996, 32(8): 785-790.

Download:  PDF(457KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The dynamically mechanical properties of Zn-22%Al alloys were measured with the low-frequency forced vibration mode by systematically changing the temperature varing rate and vibration frequency during eutectoid decomposition process. The experimental results indicated that the loss elastic modulus had different temperature varying rate and vibration frequency dependent behaviour from the storage elastic modulus, and the dependence of internal friction on temperature varying rate and vibration frequency has been discussed in the viewpoint of the complex elastic modulus. To analyse the complex elastic modulus may be more helpful to study the first-order phase transition than to only analyse internal friction.
Key words:  internal friction      complex elastic modulus      eutectoid decomposition      mechanical property      interface      Zn-Al alloy Correspondent LIU Junmin      (Department of Physics      Zhongshan University      Guangzhou 510275)     
Received:  18 August 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I8/785

1ZhangJX,PungPCW,ZengWG.PhysRev,1995;B52:268ZhangJX,YangZY,FungPCW.PhysRev,1995;B52:2782DelormeJF,SchidR,RobinR,GobinP.JPhysColloq,1971;32(C2):1013DejongheW,BatistDR,DeleayL.ScrMetall,1976;10:11254王业宁,杨正举,祝和,马进超.南京大学学报(自然科学版),1963;2:15马应良,葛庭燧.物理学报,1963;20:7216张进修,罗来忠.物理学报,1988;37:353,3637WangYN,ChenXiaohua,ShenHuimin.In:KeTSed.,ProcIntConfonInternalFrictionandUltrasonicAttenuationinSolids,Beijing:AcademicPublishers,1989:3058BidauxJE,SchalierR,BenoitW.ActaMetall,1989;37:8039LiuHY,JonesH.ActaMetallMater,1992;40:200310NuttalK.JInstMet,1971;99:26611TorisakaY,KojimaS.ActaMetallMater,1991;39:94712刘军民,张进修.物理学报,待发表13NowickAS,BerryBS.AnelasticRelaxationinCrystallineSolids.NewYork:AcademicPress,1972:24714HermidaEB.PhysStatusSolidi,1993;B178:371
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[3] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[4] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[5] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[6] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[7] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[8] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[9] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[10] WANG Furong, ZHANG Yongmei, BAI Guoning, GUO Qingwei, ZHAO Yuhong. First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface[J]. 金属学报, 2023, 59(6): 812-820.
[11] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
[12] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[13] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[14] LI Shujun, HOU Wentao, HAO Yulin, YANG Rui. Research Progress on the Mechanical Properties of the Biomedical Titanium Alloy Porous Structures Fabricated by 3D Printing Technique[J]. 金属学报, 2023, 59(4): 478-488.
[15] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
No Suggested Reading articles found!