| MICROSTRUCTURE AND MAGNETIC PROPERLY OF Fe_x(In_2O_3)_(1-x) MAGNETIC GRANULAR FILMS |
| ZHANG Liansheng; ZHANG Lin; ZHANG Ruzhen; LIU Yihua; ZHANG Weixian;HUANG Baoxin(Department of Physics; Shandong University; Jinan 250100)Correspondent: ZHANG Liansheng; associate professor Tel:(0531)8567032; Fax: (0531)8565167;E-mail: xmliu@sdu.edu.cn |
|
Cite this article:
ZHANG Liansheng; ZHANG Lin; ZHANG Ruzhen; LIU Yihua; ZHANG Weixian;HUANG Baoxin(Department of Physics; Shandong University; Jinan 250100)Correspondent: ZHANG Liansheng; associate professor Tel:(0531)8567032; Fax: (0531)8565167;E-mail: xmliu@sdu.edu.cn. MICROSTRUCTURE AND MAGNETIC PROPERLY OF Fe_x(In_2O_3)_(1-x) MAGNETIC GRANULAR FILMS. Acta Metall Sin, 1998, 34(10): 1095-1098.
|
|
|
Abstract Metal/semiconductor Fex (In2O3)1-x granular films were prepared by the rfsputtering. The microstructure was studied by using XRD, TEM and magnetic measurements.The results showed that the nanometer-sized Fe particles uniformly dispersed in the amorphousIn2O3. Appropriate annealing leads to the crystallization of In2O3 films and the growth of theFe particle size. As a result, the magnetic behavior of the films transits from superparamagneticto ferromagnetic. The variation of the lattice constant for In2O3 depends on the volume fractionof Fe particles.
|
|
Received: 18 October 1998
|
1Wang J Q, Xiao G. Phys Rev, 1994; 49B: 3982 2Chien C L.Ann Rev Mater Sci,1995;25:129 3Vink T J, Walrave W, Daams J L C, Baarslag P C, van den Meerakker J E A M. Thin Solid Films,1995; 266:145 4Shigerato Y, Takaki S, Haranou T. Appl Surf Sci, 1991; 48/49: 2699 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|