Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (10): 1095-1098    DOI:
Current Issue | Archive | Adv Search |
MICROSTRUCTURE AND MAGNETIC PROPERLY OF Fe_x(In_2O_3)_(1-x) MAGNETIC GRANULAR FILMS
ZHANG Liansheng; ZHANG Lin; ZHANG Ruzhen; LIU Yihua; ZHANG Weixian;HUANG Baoxin(Department of Physics; Shandong University; Jinan 250100)Correspondent: ZHANG Liansheng; associate professor Tel:(0531)8567032; Fax: (0531)8565167;E-mail: xmliu@sdu.edu.cn
Cite this article: 

ZHANG Liansheng; ZHANG Lin; ZHANG Ruzhen; LIU Yihua; ZHANG Weixian;HUANG Baoxin(Department of Physics; Shandong University; Jinan 250100)Correspondent: ZHANG Liansheng; associate professor Tel:(0531)8567032; Fax: (0531)8565167;E-mail: xmliu@sdu.edu.cn. MICROSTRUCTURE AND MAGNETIC PROPERLY OF Fe_x(In_2O_3)_(1-x) MAGNETIC GRANULAR FILMS. Acta Metall Sin, 1998, 34(10): 1095-1098.

Download:  PDF(954KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Metal/semiconductor Fex (In2O3)1-x granular films were prepared by the rfsputtering. The microstructure was studied by using XRD, TEM and magnetic measurements.The results showed that the nanometer-sized Fe particles uniformly dispersed in the amorphousIn2O3. Appropriate annealing leads to the crystallization of In2O3 films and the growth of theFe particle size. As a result, the magnetic behavior of the films transits from superparamagneticto ferromagnetic. The variation of the lattice constant for In2O3 depends on the volume fractionof Fe particles.
Key words:  metallic granular film      microstructure      semiconductor      super-paramagnetism     
Received:  18 October 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I10/1095

1Wang J Q, Xiao G. Phys Rev, 1994; 49B: 3982
2Chien C L.Ann Rev Mater Sci,1995;25:129
3Vink T J, Walrave W, Daams J L C, Baarslag P C, van den Meerakker J E A M. Thin Solid Films,1995; 266:145
4Shigerato Y, Takaki S, Haranou T. Appl Surf Sci, 1991; 48/49: 2699
[1] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[4] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[5] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[6] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[11] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[14] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
[15] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
No Suggested Reading articles found!