| INVESTIGATION ON MICROSTRUCTURE AND SUPERPLASTICITY OF A NiAL-BASED MULTIPHASE ALLOY |
| CHEN Rongshi;GUO Jianting;YIN Weimin;ZHOU Jiyang (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Department of Materials Engineering; Dalian University of Technology;Dalian 116023) |
|
Cite this article:
CHEN Rongshi;GUO Jianting;YIN Weimin;ZHOU Jiyang (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Department of Materials Engineering; Dalian University of Technology;Dalian 116023). INVESTIGATION ON MICROSTRUCTURE AND SUPERPLASTICITY OF A NiAL-BASED MULTIPHASE ALLOY. Acta Metall Sin, 1998, 34(11): 1121-1125.
|
|
|
Abstract The microstructure of a NiAl-based multiphase alloy with a composition of Ni-25Al-25Cr has been investigated, which consists of NiAl matrix surrounded by a eutectic of α-Cr, β-Ni(Al,Cr) and γ'-Ni3(Al,Cr), and a large amount of α-Cr precipitates distributed uniformly in NiAl matrix. This alloy exihibits superplasticity elongation as high as up to 480% at 1123-1223 K and strain rates of 2.2×10-4 -3.3×10-2 s-1. The fracture after superplasticity deformation results from cavities generated by grain boundary sliding and cleavage in the grains, the mechanism for superplasticity has also been discussed.
|
|
Received: 18 November 1998
|
| 1 Johnson D R,Chen X F,Oliver B F,Noebe R D,Winttenberger J D. Intermetallics,1995;3:99 2 Yang J M,Seng S M,Bain K,Amatos R.Acta Mater,1997 45(1):295 3 Oikawa M、 Hanada S, Sakai T, Watiinabe S Mate,Trans JIM, 1995 36(9):1140 4 Fukutomi H. Harting C、 Mecking H. Z Metallk. 199O; 81: 272 5 Yang H S,Zelin M M,Muknejee A K In:Baker I, Darolia R,Whittenberger R.Yoo J D,Pittsburgh Veds High Temperature Ordered Intermetallics Alloy PE:MRS, 1993: 837 6 Li D Q, Shan A D, Liu Y, Lin T L. Scr, Metall Mate,; 1995; 33(4): 681 7 Li D Q、 Shan A D, Chen M W. Acta Metall Sin(Eng Lett), 1995; 8:419 8 Kim W Y, Hanada S, Takasugi T Scr Mater,1997; 37(7): 1053 9 Fujino S; Karoishgi N, Yoshino M, Mukai T, Okanda Y, Higashi K. Scr Mater, 1997: 37(5): 673 10Bakshi P K, Kashyap B P. J Mater Sci. 1995 30: 5065 11 Uan J Y, Chen L H, Lui T S Metall Mater Trans, 1997; 28A: 401 12 Villars P,Prince A,Dakainooto H.Handbook of Ternary Alloy Phase Diagrams,Second Printing.TheMaterials Information Society.1997:3151 13余宗森,田中卓.金属物理.北京:冶金工业出版社.1982:337(Yu Z S,Tian Z Z.Metal Physics.Beijing:The Metallurgical Industry Press,1982:337)8 |