INVESTIGATION ON MICROSTRUCTURE AND SUPERPLASTICITY OF A NiAL-BASED MULTIPHASE ALLOY
CHEN Rongshi;GUO Jianting;YIN Weimin;ZHOU Jiyang (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Department of Materials Engineering; Dalian University of Technology;Dalian 116023)
Cite this article: 

CHEN Rongshi;GUO Jianting;YIN Weimin;ZHOU Jiyang (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Department of Materials Engineering; Dalian University of Technology;Dalian 116023). INVESTIGATION ON MICROSTRUCTURE AND SUPERPLASTICITY OF A NiAL-BASED MULTIPHASE ALLOY. Acta Metall Sin, 1998, 34(11): 1121-1125.

Download:  PDF(1862KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The microstructure of a NiAl-based multiphase alloy with a composition of Ni-25Al-25Cr has been investigated, which consists of NiAl matrix surrounded by a eutectic of α-Cr, β-Ni(Al,Cr) and γ'-Ni3(Al,Cr), and a large amount of α-Cr precipitates distributed uniformly in NiAl matrix. This alloy exihibits superplasticity elongation as high as up to 480% at 1123-1223 K and strain rates of 2.2×10-4 -3.3×10-2 s-1. The fracture after superplasticity deformation results from cavities generated by grain boundary sliding and cleavage in the grains, the mechanism for superplasticity has also been discussed.

Key words:  NiAl      superplasticity      microstructure      fracture mechanism      NiAl      superplasticity      microstructure      fracture mechanism     
Received:  18 November 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I11/1121

1 Johnson D R,Chen X F,Oliver B F,Noebe R D,Winttenberger J D. Intermetallics,1995;3:99
2 Yang J M,Seng S M,Bain K,Amatos R.Acta Mater,1997 45(1):295
3 Oikawa M、 Hanada S, Sakai T, Watiinabe S Mate,Trans JIM, 1995 36(9):1140
4 Fukutomi H. Harting C、 Mecking H. Z Metallk. 199O; 81: 272
5 Yang H S,Zelin M M,Muknejee A K In:Baker I, Darolia R,Whittenberger R.Yoo J D,Pittsburgh Veds High Temperature Ordered Intermetallics Alloy PE:MRS, 1993: 837
6 Li D Q, Shan A D, Liu Y, Lin T L. Scr, Metall Mate,; 1995; 33(4): 681
7 Li D Q、 Shan A D, Chen M W. Acta Metall Sin(Eng Lett), 1995; 8:419
8 Kim W Y, Hanada S, Takasugi T Scr Mater,1997; 37(7): 1053
9 Fujino S; Karoishgi N, Yoshino M, Mukai T, Okanda Y, Higashi K. Scr Mater, 1997: 37(5): 673
10Bakshi P K, Kashyap B P. J Mater Sci. 1995 30: 5065
11 Uan J Y, Chen L H, Lui T S Metall Mater Trans, 1997; 28A: 401
12 Villars P,Prince A,Dakainooto H.Handbook of Ternary Alloy Phase Diagrams,Second Printing.TheMaterials Information Society.1997:3151
13余宗森,田中卓.金属物理.北京:冶金工业出版社.1982:337(Yu Z S,Tian Z Z.Metal Physics.Beijing:The Metallurgical Industry Press,1982:337)8

[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[3] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[4] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[5] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[6] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[7] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[11] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[14] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
[15] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
No Suggested Reading articles found!