| THE PREFERRED ORIENTATION, MICROSTRUCTURE AND MAGNETOSTOSTRION IN DIRECTIONALLX SOLIDIFIED TbDyFe ALLOYS |
| JIANG Chengbao (Department of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083)ZHOU Shonseng;ZHANG Maocai;WANG Run (State Key Laboratory for Advanced Metal Materials; University of Science and Technology Beijing; Beijing 100083) |
|
Cite this article:
JIANG Chengbao (Department of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083)ZHOU Shonseng;ZHANG Maocai;WANG Run (State Key Laboratory for Advanced Metal Materials; University of Science and Technology Beijing; Beijing 100083). THE PREFERRED ORIENTATION, MICROSTRUCTURE AND MAGNETOSTOSTRION IN DIRECTIONALLX SOLIDIFIED TbDyFe ALLOYS. Acta Metall Sin, 1998, 34(2): 164-170.
|
|
|
Abstract The device of zone melting directional solidification has been used to investigate the preferred orientation, microstructure and magnetostriction of Tb0.3Dy0.7(Fe, M)1.95 (M=Al,Mn, B) metallic compound. When the temperature gradient GL≈700 K/cm, the growth velocity V mm/min, the crystal grows in plannar interface, 1< V 6 mm/min, in cellular morphology; V=8 - 12 mm/min, in primary dendrite; V > 15 mm/min, in developed delldrite. As V=12 mm/min, GL≈1000 and 400 K/cm, the crystal grows in cellular morphology developed dendrite, respectively. Crystals in cellular morphology are <110> preferred orientation and poor magnetostrictive property. Crystals in primary dendrite with <112> preferred orientation, have a good performance, the maximum value of magnetostriction (A) is 0.00175. Crystals in developed dendrite with part <112> orientation have an inferior property than the former.
|
|
Received: 18 February 1998
|
1Teter J P, Clark A E.J Appl Phgs, 1987; 61: 3787 2Westwood P, Abell J S, Pitman K C.J Appl Phys, 1990; 67: 4998 3蒋成保.北京科技大学博士学位论文,1996 (Jiang C B. Doctor Thesis, Universty Science and Technology Beijing, 1996) 4Weinberg F, Chalmers B. Can J Phys, 1951; 29: 382 5安阁英,刘立新.金属科学与工艺,1985;14:55 (A G Y, Li: L X. Metal Sci Technol, 1985; 14: 55) 6Flemings M C. Solidification Processing, 1974: 58 7Jiang C B, Zhou S Z, Wang R. Acta Metall Mater to be published |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|