THE HIGH TEMPERATURE TENSILE BEHAVIORS OF Al_(67)Ti_(25)Mn_8 INTERMETALLICS UNDER DIFFERENT STRAIN RATES
SUN Jian; FU Yunyi; SHI Rong; SUN Xiaoguang; HU Gengxiang (The Public Laboratory of State Education Commission for High Temperature Materials & High Temperature Tests; Shanghai Jiaotong University; Shanghai 200030)
Cite this article:
SUN Jian; FU Yunyi; SHI Rong; SUN Xiaoguang; HU Gengxiang (The Public Laboratory of State Education Commission for High Temperature Materials & High Temperature Tests; Shanghai Jiaotong University; Shanghai 200030). THE HIGH TEMPERATURE TENSILE BEHAVIORS OF Al_(67)Ti_(25)Mn_8 INTERMETALLICS UNDER DIFFERENT STRAIN RATES. Acta Metall Sin, 1998, 34(5): 526-530.
Abstract The tensile tests of Al67Ti25Mn8 intermetallic compound were performed at 1173 K and at the range of strain rates from 3.34×10-5 to 6.68× 10-4 s-1. The results show that with decreasing strain rates, the yield stress decreases and the tensile ductility increases from 2.8% to 21%. The good high temperature ductility at low strain rates is attributed to dynamic recovery and dynamic recrystallization during deformation. The fractured surfaces of this compound are intergranular, which suggests that the grain boundaries of this alloy are also intrinsic weak.
1Hu G X, Chen S P, Wu X H, Chen X F J Mater Res, 1991;6: 957 2Kumar K S and Brown S A Philos Mag,1992;65:91 3Hu G X,Chen S P,Wu X H,Rong Y H;Chen X F Proc of the Int Workshop of Ordered Intermetallics,Hangzhou,1992:78 4Brown S A, Kumar K S. Scr Metall Matet 1990; 24: 505 5Kumar K S,Brown S A.Intermetallics,1996;4:231 6Vedula K,Stephens J R. Mater Res Soc Symp Proc,1987 81:381 7Taksugi T, Rikukawa S, Hanada S. Acta Metall Mater, 1992; 40: 1895N