THE IMPEDANCE ANALYSIS OF REACTION KINETICS AT THE INTERFACE OF MOLTEN Sn-S/ZnCl_2-NaCl SYSTEM
WANC Shulan; LI Guangqiang; SUI Zhitong (School of Materials and Metallurgy; Northeastern University; Shenyang 110006)
Cite this article: 

WANC Shulan; LI Guangqiang; SUI Zhitong (School of Materials and Metallurgy; Northeastern University; Shenyang 110006). THE IMPEDANCE ANALYSIS OF REACTION KINETICS AT THE INTERFACE OF MOLTEN Sn-S/ZnCl_2-NaCl SYSTEM. Acta Metall Sin, 1998, 34(5): 521-525.

Download:  PDF(363KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The interfacial desulphurization reaction kinetics between molten Sn-S alloy and ZnCl2-NaCl salt was studied by an AC impedance method and the impedance response of this system was given. By using Randles equivalent circuit, the kinetic factors on electrode reaction between the alloy and the salt were obtained, such as electrolyte resistance Re, double-layer capacitance Cd, charge transfer resistance Rct, rate constant of desulfurization reaction Kf and so on. When overpotential η equals to -85 mV, these values are Re=2.93×10-5 Ω.m2, Rct =2.47×10-5 Ω.m2, Cd=1.01 F/m2, Kf=2.1 × 10-3 s-1, respectively.
Key words:  AC impedance method      Randles equivalent circuit      charge-transfer resistance      double-layer capacitance      salt-metal interfacial reaction     
Received:  18 May 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I5/521

1蒋国昌,徐匡迪,邓健雄.金属学报,1990;26:B33(Jiang Guochang, Xu Kuangdi, Deng Jianxiong. Acta Metall Sin, 1990 26: B33)
2Xu C S, Tang X. ISIJ Int, 1992; 32: 1081
3焉毓璋,兰洪.金属学报,1991; 27:B224(Yan Yuzhang,Lan Hong.Acta Metall Sin,1991; 27:B224)
4 Ross Macdonald J.Applications of Impedance Spectroscopy Newyork:Wirey—Interscience Publication,1987
5Hino M, Nitta T, Chida S, Banya S Proc 3rd Int Conf on Molten Slags and Fluexs, London: The Inst Met,1988:286
6Gabrielli C.Identification of Electrochemical Processes by Frequency Response Analysis,Technical Report Number 004/83;Solartron Instrument,A Division of Schlumberger Electroniocs (UK)Ltd.1984;2:15
7小野阳一,石飞精助,铁钢,1977;60:1533(Ono YOichi, Ishitobi Seisuke.Tetsu Hagane;1974 60: 1533)
8 Khodov N V; Alfortsev V M, Danilin L A. Tszetnaya Metaplugiya,1987 4: 113
No related articles found!
No Suggested Reading articles found!