Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (5): 506-510    DOI:
Current Issue | Archive | Adv Search |
TEXTURE CHARACTERISTICS OF Fe-6.5%Si SHEETS PRODUCED BY THE DEPOSITIONDIFFUSION METHOD
HU Guangyong; ZUO Liang; WU Baolin; WANG Gang; LIANG Zhide (School of Materials and Metallurgy; Northeastern University; Shenyang 110006)
Cite this article: 

HU Guangyong; ZUO Liang; WU Baolin; WANG Gang; LIANG Zhide (School of Materials and Metallurgy; Northeastern University; Shenyang 110006). TEXTURE CHARACTERISTICS OF Fe-6.5%Si SHEETS PRODUCED BY THE DEPOSITIONDIFFUSION METHOD. Acta Metall Sin, 1998, 34(5): 506-510.

Download:  PDF(443KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Fe-6.5%Si samples were prepared from cold-rolled Fe-3%Si sheets by the deposition-diffusion method. The Si concentrations of the deposited samples with and without homogenization were examined by the X-ray diffraction technique. The texture characteristics of the cold-rolled, deposited and homogenized samples were evaluated by the ODF analysis. It was shown that after deposition the typical cold-rolling textures were weakened to a large extent while the η-fiber (<001>//RD)with the maximum density at the {120}<001>component became dominated.After homogenization the {120}<001>component evolved into{130}<001>for the conventional cold-rolled samed sample with 0.9 mm thickness but it kept strongest for the cross-shear cold-rolled sample with 0.35 mm thickness.
Key words:  FE-6.5%Si sheet      deposition -diffusion mehtod       texture      cross-shear rolling     
Received:  18 May 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I5/506

1Ruder W E. Proc Inst Radio Ena, 1942 30: 437
2津屋.荒井贤一.固体物理,1978;13:237(Tsuya Noboru,Arai Kenichi.Solid State Phys,1978;13:237)
3Takat: Y J Appl Phys, 1988; 64: 5367
4Ames S L, House J, Bitler W R. J Appl Phys, 1969; 40: 1577
5山路常弘,和田守弘,材料,1993;6:1824(Kasai Shyokou, Wada Morihiro. CAMP—ISIJ; 1993 6: 1824)
6朱泉.钢铁,1980;15:1(Zhu Quan .Iron and Steel,1980;15:1)
7梁志德,徐家桢,王福,织构材料的三维取向分析术-ODF分析.沈阳:东北工学院出版社,1986:36(Liang Zhide;Xu Jiazhen,Wang Fu.Three Dimensional Orientation Analysis of Textured Materials-ODF Analysis. Shenyang:Northeast University of Technology Press,1986:36)
8孔德谆.化学热处理原理.北京:航空工业出版社,1992:9 (Kong Dezhun.Principles of Chemical Heat Treatment.Beijing:Aeronautical Industry Press,1992:9)
9虞觉奇,罗文质,陈邦迪,陈洪鉴.二元合金状态图集.上海:上海科学技术出版社,1987: 375(Yu Jueqi,Luo Wenzhi,Chen Bangdi,Chen Hongjian.Collections of Phase Diagrams of Binary Alloys.Shanghai:Shanghai Science and Technology Press,1987:375)
[1] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[2] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[3] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[4] YANG Ping, WANG Jinhua, MA Dandan, PANG Shufang, CUI Feng'e. Influences of Composition on the Transformation-Controlled {100} Textures in High Silicon Electrical Steels Prepared by Mn-Removal Vacuum Annealing[J]. 金属学报, 2022, 58(10): 1261-1270.
[5] DING Ning, WANG Yunfeng, LIU Ke, ZHU Xunming, LI Shubo, DU Wenbo. Microstructure, Texture, and Mechanical Properties of Mg-8Gd-1Er-0.5Zr Alloy by Multi-Directional Forging at High Strain Rate[J]. 金属学报, 2021, 57(8): 1000-1008.
[6] YAN Mengqi, CHEN Liquan, YANG Ping, HUANG Lijun, TONG Jianbo, LI Huanfeng, GUO Pengda. Effect of Hot Deformation Parameters on the Evolution of Microstructure and Texture of β Phase in TC18 Titanium Alloy[J]. 金属学报, 2021, 57(7): 880-890.
[7] ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang. Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys[J]. 金属学报, 2021, 57(11): 1396-1415.
[8] XU Zhanyi, SHA Yuhui, ZHANG Fang, ZHANG Huabing, LI Guobao, CHU Shuangjie, ZUO Liang. Orientation Selection Behavior During Secondary Recrystallization in Grain-Oriented Silicon Steel[J]. 金属学报, 2020, 56(8): 1067-1074.
[9] YU Lei,LUO Haiwen. Effect of Partial Recrystallization Annealing on Magnetic Properties and Mechanical Properties of Non-Oriented Silicon Steel[J]. 金属学报, 2020, 56(3): 291-300.
[10] CHENG Chao,CHEN Zhiyong,QIN Xushan,LIU Jianrong,WANG Qingjiang. Microstructure, Texture and Mechanical Property ofTA32 Titanium Alloy Thick Plate[J]. 金属学报, 2020, 56(2): 193-202.
[11] DU Zijie, LI Wenyuan, LIU Jianrong, SUO Hongbo, WANG Qingjiang. Study on the Uniformity of Structure and Mechanical Properties of TC4-DT Alloy Deposited by CMT Process[J]. 金属学报, 2020, 56(12): 1667-1680.
[12] Liping DENG,Kaixuan CUI,Bingshu WANG,Hongliang XIANG,Qiang LI. Microstructure and Texture Evolution of AZ31 Mg Alloy Processed by Multi-Pass Compressing Under Room Temperature[J]. 金属学报, 2019, 55(8): 976-986.
[13] Xin LI,Yuecheng DONG,Zhenhua DAN,Hui CHANG,Zhigang FANG,Yanhua GUO. Corrosion Behavior of Ultrafine Grained Pure Ti Processed by Equal Channel Angular Pressing[J]. 金属学报, 2019, 55(8): 967-975.
[14] Zheng LIU,Jianrong LIU,Zibo ZHAO,Lei WANG,Qingjiang WANG,Rui YANG. Microstructure and Tensile Property of TC4 Alloy Produced via Electron Beam Rapid Manufacturing[J]. 金属学报, 2019, 55(6): 692-700.
[15] Houlong LIU,Mingyu MA,Lingling LIU,Liangliang WEI,Liqing CHEN. Effect of Hot Band Annealing Processes on Texture and Formability of 19Cr2Mo1W Ferritic Stainless Steel[J]. 金属学报, 2019, 55(5): 566-574.
No Suggested Reading articles found!