KINETICS OF DESULPHURIZATION BY POWDER INJECTION AND BLOWING IN RH REFINING OF MOLTEN STEEL
WEI Chiho;ZHU Shoujun; YU Nengwen (Shanghai Enhanced Laboratory of Ferrous Metallurgy; Shanghai University; Shanghai 200072)
Cite this article: 

WEI Chiho;ZHU Shoujun; YU Nengwen (Shanghai Enhanced Laboratory of Ferrous Metallurgy; Shanghai University; Shanghai 200072). KINETICS OF DESULPHURIZATION BY POWDER INJECTION AND BLOWING IN RH REFINING OF MOLTEN STEEL. Acta Metall Sin, 1998, 34(5): 497-505.

Download:  PDF(735KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The desulphurization process by powder injection and blowing in RH refining of molten steel and its mechanism have been considered and analyzed. Based on the two-resistance mass transfer theory and the mass balance of sulphur in the system, a kinetic model for the process has been developed. The ralated parameters of the model have been determined. Calculating and modelling for the process by injecting and blowing the lime based powder flux under the assumed operating modes in a RH degasser of 300 t capacity have been carried out using the model. The corresponding circulation rate and the powder injection and blowing rate were taken as 100 t/min and 150 kg/min, respectively. The initial contents of sulphur and the amounts of powder injection and blowing were respectively assumed to be 70, 60, 50, 40, 30, 20×10-4% (massfraction) and 10, 8, 6, 5, 4, 3 kg/t-steel. The total treatment time for desulphurization under each mode was set up to be 24 min that is equivalent to eight circulation cycles of liquid steel to be treated. The results indicated that the prediction made by this model is in good agreement with some data of the industrial experiments and production practice, injecting and blowing the lime-based powder flux(85%CaO+15%CaF2)of 3-5 kg/t-steel with the total treatment time of 12-20 min, it is entirely possible to make the sulphur content in molten steel decrease to the ultra-low level below (5- 10)× 10-4% from (60-80)×10-4%; intensifying the powder injection and blowing operation and increasing the circulation rate of liquid steel may effectively raise the rate of the process in RH refining.
Key words:  RH refining      desulphurization by powder injection and blowing      lime-base powder flux      kinetics     
Received:  18 May 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I5/497

1远藤公一.制铁研究,19892 335:20(Endoh K. Sada Tetsu Togisata,1989; 335:20)
2 Endoh K.Nippon Steel Technic Rep,1990;45(4)
3Hatakeyama T,Mizukami Y,Igo K,Oita M.Ircn&Steelmaker,1989;15(7):23
4 Myrayama N,Mizukami Y,Azuma K,Onoyma S,Imais T.Proc 6th International Iron and Steel Congress,Vol.3, Napoya: The Iron and Steel Institute of Japan, 1990 151
5 Hale R J,Merk R,Otterman B A Steelmaking Conf Proc,ISS-AIME,Detroit,MI,1990:69
6上原搏英,水藤正人,高桥清志,有吉政弘,桐原理,加藤嘉英。CAMP-ISIJ,1922 5:1240(Ueharal H.Suito M,Takahashi K,Ariyoshi S,Kirihara T,Kato Y.CAMP-ISIJ,1992; 5:1240)
7冈田泰和,深川信,家田幸治,海老原明彦,池宫洋行,真目薰CAMP—ISIJ, 1992;5:1238(Okada Y, Fukawa M, Yata K, Ebihara A, Ikemiya N, Makoto M CAMP—ISIJt 1992 5: 1238)
8冈田泰和,真屋敬一。铁钢,1994;80(1):T9(Okada Y. Shinya H. Tetsu Hagane, 1994; 80(1): T9)
9川合保治,森克已,三宫好史。铁钢,1975;61(1):29(Kawai Y,Mori K,Sanomiya Y.Tetsu Hagane.1975;61(1):29)
10 Oeters F, Strohmenger P, Pluschkell W Arch Eisenhuttenwes, 1973 44: 727
11溶铁·溶滓物性植便览,溶钢·溶滓部会报告,东京:日本铁钢协会,1971:70(Youtetsu.Youkasu No MonoshoUe Yasukata ,YouHagane.Youkasu Tomokazu TsuguNori,Tokyo:ISIJ,1971:70)
12Tsujino R, Nakashima J, Hirai M, Sawada I. ISIJ Int; 1989: 29(7):589
13Szatkowshi M,Tsai M C.Ironmaking Steelmaking,1991;17(4):65
14 Geiger G H,Poirier D R.Transport Phenomena in Metallurgy,Reading Mass:Addison-Wesley;1973:18
15饭田孝道,上田满,森田普一郎.铁钢,1977;63(4):163(Handa N,Kamita M,Morita H,Tetsu Hagane,1977; 63(4):163)
16 Komai T,Mizukami Y, Proc 7th International Conference on Vacuum Metallurgy,Tokyo:ISIJ,1982:1383
17桐原理,加藤嘉英,田口整司,藤井辙也,上原搏英,大宫茂CAMP—ISIJ,1992; 5:1239(Kirihara T, Kato Y, Taguchi H, Fujii W, Uehara H, Osora S. CAMP-ISIJ, 1992; 5: 1239)
[1] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[2] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[3] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[4] LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang. Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation[J]. 金属学报, 2023, 59(10): 1376-1388.
[5] DU Zonggang, XU Tao, LI Ning, LI Wensheng, XING Gang, JU Lu, ZHAO Lihua, WU Hua, TIAN Yucheng. Preparation of Ni-Ir/Al2O3 Catalyst and Its Application for Hydrogen Generation from Hydrous Hydrazine[J]. 金属学报, 2023, 59(10): 1335-1345.
[6] GUO Lu, ZHU Qianke, CHEN Zhe, ZHANG Kewei, JIANG Yong. Non-Isothermal Crystallization Kinetics of Fe76Ga5Ge5B6P7Cu1 Alloy[J]. 金属学报, 2022, 58(6): 799-806.
[7] TANG Shuai, LAN Huifang, DUAN Lei, JIN Jianfeng, LI Jianping, LIU Zhenyu, WANG Guodong. Co-Precipitation Behavior in Ferrite Region During Isothermal Process in Ti-Mo-Cu Microalloyed Steel[J]. 金属学报, 2022, 58(3): 355-364.
[8] XU Kun, WANG Haichuan, KONG Hui, WU Zhaoyang, ZHANG Zhan. Precipitation Kinetics of Al3Sc in Aluminum Alloys Modeled with a New Grouping Cluster Dynamics Model[J]. 金属学报, 2021, 57(6): 822-830.
[9] ZHU Min, OUYANG Liuzhang. Kinetics Tuning and Electrochemical Performance of Mg-Based Hydrogen Storage Alloys[J]. 金属学报, 2021, 57(11): 1416-1428.
[10] LIU Feng, WANG Tianle. Precipitation Modeling via the Synergy of Thermodynamics and Kinetics[J]. 金属学报, 2021, 57(1): 55-70.
[11] Shuaipeng WANG, Wenhua LUO, Gan LI, Haibo LI, Guangfeng ZHANG. Effect of La Content on Hydriding Kinetics of Ce-La Alloys[J]. 金属学报, 2018, 54(8): 1187-1192.
[12] Shixin XU, Wei YU, Shujia LI, Kun WANG, Qisong SUN. Effects of Pre-Deformation Temperature on Nanobainite Transformation Kinetics and Microstructure[J]. 金属学报, 2018, 54(8): 1113-1121.
[13] Ke ZHANG, Xinjun SUN, Mingya ZHANG, Zhaodong LI, Xiaoyu YE, Zhenghai ZHU, Zhenyi HUANG, Qilong YONG. Kinetics of (Ti, V, Mo)C Precipitated in γ /α Matrix of Ti-V-Mo Complex Microalloyed Steel[J]. 金属学报, 2018, 54(8): 1122-1130.
[14] Yin BAI, Zhengdong LIU, Jianxin XIE, Hansheng BAO, Zhengzong CHEN. Effect of Pre-Oxidation Treatment on the Behavior of High Temperature Oxidation in Steam of G115 Steel[J]. 金属学报, 2018, 54(6): 895-904.
[15] Hao CHEN, Congyu ZHANG, Jianing ZHU, Zenan YANG, Ran DING, Chi ZHANG, Zhigang YANG. Austenite/Ferrite Interface Migration and Alloying Elements Partitioning: An Overview[J]. 金属学报, 2018, 54(2): 217-227.
No Suggested Reading articles found!