Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (6): 633-639    DOI:
Current Issue | Archive | Adv Search |
MICROSTRUCTURE,DIFFUSION ACCUMULATION OF HYDROGEN AND CRACKING BEHAVIOR IN THE INTERFACE BETWEEN CLADDING AND BASE METALL
TENG Qinghai; CHEN Lian; LIU Di;; KE Wei(Institute of Corrosion and Protection of Metal; The Chinese Academy of Sciences; State Key Laboratory forCorrosion and Protection; Shenyang 110015)( Institute of Metal Research; The Chinese Academy of Sciences; Liaoning Key Laboratory for Material andHydrogen; Shenyang 110015)( Institute of Equipmeat;Research Fushun Petrochemical Company; Fushun )(Correspondednt : MENC Qinghai; Tel: (0413)B434819; Tel. (0413)2425835
Cite this article: 

TENG Qinghai; CHEN Lian; LIU Di;; KE Wei(Institute of Corrosion and Protection of Metal; The Chinese Academy of Sciences; State Key Laboratory forCorrosion and Protection; Shenyang 110015)( Institute of Metal Research; The Chinese Academy of Sciences; Liaoning Key Laboratory for Material andHydrogen; Shenyang 110015)( Institute of Equipmeat;Research Fushun Petrochemical Company; Fushun )(Correspondednt : MENC Qinghai; Tel: (0413)B434819; Tel. (0413)2425835. MICROSTRUCTURE,DIFFUSION ACCUMULATION OF HYDROGEN AND CRACKING BEHAVIOR IN THE INTERFACE BETWEEN CLADDING AND BASE METALL. Acta Metall Sin, 1998, 34(6): 633-639.

Download:  PDF(2000KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The relationships among the microstructure, diction accUmulatinn of hydrogen and hydrogen induced crabbing behavinr of the interfaCe were investigated. The eXperimental cults saal that the hydrogen distribution in the interfaCe is corresponding to its ndcrostructure,the behavior of by~n induced cracking may expressed by the theory of molecular hydrogen PreSSure. The paths where hydrogen disbonding cracks nucleated and propagated were classal into four typeS, the disbonding cracks would not penetrate into the base metal.
Key words:  cladding/matris interface      microstructure       hydrogen diffusion      hydrogen in duced cracking     
Received:  18 June 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I6/633

1 Task Group IIII of the Subco mmittee on Hydrogen Embrittlementof the Japan Pressure Vennel Rsearch Council.WRC Bulletin 1985; 305:22
2 Pressouyre G M ,Chaillet J M ,Valette G.First International Conterence on Current Solutions to the Hstudmmen Problems in steels, Washington D.C, 1982: 349
3 Sakai T, Asami K, Katsumata M, Takada H, Tanaka O. First International Conference on Current Solutions to the Hydrogen Problems in steels Washington D C,1982:340
4 Bernstein I M, Presaouyre G M. In: Oriani R A, Hirth J PI Smialowski M S eds . HudroaenDegradation of Ferrous Alloys ,,1985:641
5 Thoiano A R. Trans ASM. 1960; 52: 54
6 Telelanm A S. In: Bernstein I M, Thompson A W eds, Hgdrogen in Metal ,Metals park OH : ASM, 1974:17
7 Tada H,Paris P ,Irwin G.Stress Analysis of Cracks Handbook USA :Del Research Corp.1985:28
8 Oriani R A. Ann Rev Mater Sci 1978; 8: 327
[1] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[4] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[5] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[6] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[7] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[11] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[12] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[13] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[14] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[15] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
No Suggested Reading articles found!