OXIDATION BEHAVIOR OF THE SPUTTERED MICSOCRVSTALLNE CONATINGOF LDZ125 SUPERALLOR AT HIGH-TEMPERAFUS
ZHANG Jie; LOU Hanyi(State Key Laboratory of Corrosion and Protection ;Institute of and Protection Of Metals; The ChineseAcademy of Sciences ; Shenyang 110015)Correspondent : LOU Hanyi; professor Tel: (024)3915908; Fax: (024)3894149
Cite this article:
ZHANG Jie; LOU Hanyi(State Key Laboratory of Corrosion and Protection ;Institute of and Protection Of Metals; The ChineseAcademy of Sciences ; Shenyang 110015)Correspondent : LOU Hanyi; professor Tel: (024)3915908; Fax: (024)3894149. OXIDATION BEHAVIOR OF THE SPUTTERED MICSOCRVSTALLNE CONATINGOF LDZ125 SUPERALLOR AT HIGH-TEMPERAFUS. Acta Metall Sin, 1998, 34(6): 627-632.
Abstract The microcrystalline LDZ125 coating producted by planar magnetron sputteredtechnique has very fine grain size(less than 100 urn) and homogeneous structure consisting ofγ--Phase, while the cast alloy is composed of 7, 7' and Carbides. The oxalation resistance ofthe ~Crystalline layer was much better than that of the CaSt LDZ125 alloy. The Oalde scalesformed on the cast LDZ125 alloy was composed of AJZO3 with small ~s of Cr, Ti and Nieddes. ~ 500 h Obeation, the colltelit of A12O3 in the chide scales reduce because of its spallation during exposure, and the oalde scale was mainly composed of CrZO3 and TiO2. The chidescale formed on the inicrocrystalline LDZ125 consists of Only o--AJsos which had excellent ad-hesion and did hot spall in the durstion of exposure. The beneficial ears of ndcrocrystallizstionon the O~ion resistance of the superalloy were discussed.
1 Whittle D P,In:Coutsouradis D ,Felix P, Fischmeister H ,Habraken L Lindblom Y,Speidel M O eds . High Temp Alloys for Gas Turbines ,London :Appl Sci 1978:109 2 Felix P. In: Hart A B, Cultler A J B eds. Dopsition and Corr. in Gas Turbines ,London: Appl. Sci, 1972:331 3 Lou Hanyi, Wang Fuhui. Oxid Met, 1992; 38: 299 4 Lou Hanyi , Wang Fuhui, Zhu Shenlong. Surf Coat Tech, 1994; 63: 1055 楼翰一,唐幼军,孙晓峰,管恒荣 金属学报,1994;30:B109 (Lou H Y, Tang Y J, Sun X F, Guan H R. Acta Metall Sin, 1994; 30: B109) 6 Lou H Y, Tang Y J, Sun X F, Guan H R, Mater Sci Eng, 1996; A207: 121 7 Wagner C Z.Electronchem 1959; 63: 772 8 Karch J ,Birringer R ,Gleiter H.Nature ,1987;330:556