Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (6): 655-660    DOI:
Current Issue | Archive | Adv Search |
STRUCTURE AND MICROTRIBOLOGICAL BEHAVIOR OF TEFLON/ Si_3N_4 MICRO-ASSEMBLING FILM
WANC Jihui; WANG Liduo; LU Xinchun; WEN Shizhu; LI Hengde( State Key Laboratory of Tribology; Tsinghua University; Beijing 100084)( Department of Chemistry; Hong Kong University of Science and Technology; Hong Kong)Coerespondent: LU Xinchun; associate professor Tel: (010)62783160-806; Fax. (010)62784691;E-mail: xcluntl pim tsinghua edu cn
Cite this article: 

WANC Jihui; WANG Liduo; LU Xinchun; WEN Shizhu; LI Hengde( State Key Laboratory of Tribology; Tsinghua University; Beijing 100084)( Department of Chemistry; Hong Kong University of Science and Technology; Hong Kong)Coerespondent: LU Xinchun; associate professor Tel: (010)62783160-806; Fax. (010)62784691;E-mail: xcluntl pim tsinghua edu cn. STRUCTURE AND MICROTRIBOLOGICAL BEHAVIOR OF TEFLON/ Si_3N_4 MICRO-ASSEMBLING FILM. Acta Metall Sin, 1998, 34(6): 655-660.

Download:  PDF(1088KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Micro-assembling Teflon/Si3N4 multi--farer film was synthesized by ion beam alternating sputtering Teflon and Si3N4 ceramic targets. The structure, mechanical and ndcrotribological properties were studied by PHI--5300, FT--IR2000, Xos and atolinc force and frictioll force microscOPe. The results show that the multilayer is consist of crystalline Teflon and amorphous St3N4. The hardness of the multilayer is less than that of St3N4; but the toughness of Teflon/SisN' is greatly approved. This Teflon/Si3N4 multilayer has low friction coefficient and high wear resistance. The friction force of Tellon/ St3N4 film is linear with the load in nano--scale.The worn track will be formed in Teflon film when the load is greater than 70 uN.Keywrods: Teflon, multilayer film, structure, structure ,microtribology
Key words:  Teflon      multilayer film      structure      structure       microtribology     
Received:  18 June 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I6/655

1 Clegg W J, Kendall K, Alford N M, Button T W, Birchal J D. Nature , 1990; 347(4): 455
2 Matthews F L,Rawlings R D.Co mposite materials :Engineering and science ,London :Chapman & Hall press ,1994:29
3 Zhou B L.J Mater Sci Tech ,1993;9:9
4 马祖力.生物与仿生 天津科技出版社,1984:35 (Ma Z L.Organisms and Biomimetics Tianjin Press of science and tecnology ,1984: 35)
5 Vosson J L, Kerm W. Thin Film Processes, New York: Academic press, 1978: 6
6 Affinto J ,Martin P,Gross M,Coronado C,Greenwell E.Thin Solid Films 1995;270(1):514
7 Liu C H,Li W Z,Li H D,He J L.Sur coat technol ,1996;84:420
8 王吉会,路新春.温诗铸.材料研究学报,1997;11(4):351 (Wang J H, Lu X C, Wen S Z. Chin J Mater , Res, 1997; 11(4): 351)
9 Bhushan B, Gupta B K. Handbook of tribology New York: McGarw-Hill Inc, 1991; 5.34%
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[3] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[4] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[5] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[6] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[7] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[8] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[9] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[10] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[11] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[12] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[13] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[14] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[15] LI Qian, LIU Kai, ZHAO Tianliang. Rust Formation Behavior and Mechanism of Q235 Carbon Steel in 5%NaCl Salt Spray Under Elastic Tensile Stress[J]. 金属学报, 2023, 59(6): 829-840.
No Suggested Reading articles found!