NUMERICAL MICROSTRUCTURE SIMULATION OF LASER RAPID FORMING 316L STAINLESS STEEL |
JIA Wenpeng1; TONG Huiping1; HE Weiwei1; LIN Xin2; HUANG Weidong2 |
1.State Key Laboratory of Porous Metals Technologies; Northwest Institute for Nonferrous Metal Research; Xi’an 710016
2.State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi’an 710072 |
|
Cite this article:
JIA Wenpeng TONG Huiping HE Weiwei LIN Xin HUANG Weidong. NUMERICAL MICROSTRUCTURE SIMULATION OF LASER RAPID FORMING 316L STAINLESS STEEL. Acta Metall Sin, 2010, 46(2): 135-140.
|
Abstract The laser rapid forming (LRF) as an advanced solid freedom fabrication technology, has been developed rapidly in recent decade. By rapid prototyping with laser cladding, LRF realizes the direct net shaping of the components with irregular shapes and fine inner structures, and gives a short–route, low–cost and high–flexibility fabrication of aero components, aero–engine parts and biomedical implants. In the LRF, melting and solidification are happened in a dynamic non–equilibrium, high temperature gradient and rapid solidification manner, so that the microstructure of the laser rapid formed part is finer than that of ordinary cast or forge part and presents a characteristic of typical epitaxial growth. Therefore, to achieve the predict and control of the microstructure evolution is a key problem. Much efforts have been devoted to narrating the solidification and crystallization in melting pool, but little attention has been paid to stuy the microstructure of LRF part. In this paper, the evolution otemperture field and solidification of LRF part were concerned, the relationships between as–deposited microstructure and the local solidification conditions such as solidification velocity and temperaturgradient of moving melting pool were also investigeted. A coupled 2D transient finite element LRF epitaxial growth model was developed. The morphology evolution and first order dendrite arm space λ1 distribution in 2.8 mm high LRF 316L stainless steel wall were simulated. The results show that the microstructure of LRF 316L stainless steel wall is mainly columnar austenitic dendrites, and the λ1 gradually becomes larger from the bottom about 6.5 μm to the top about 17 μm which is in good agrement with te experimntal. Further more, on the basis of the validated model, morphology volution and λ1 distribution in 40 mm high LRF 316L stainless steel wall are also predicted.
|
Received: 27 March 2009
|
Fund: Supported by National Key Basic Technology R&D Program of China (No.2007BAE07B05) and National Natural Science Foundation of China (No.50331010) |
[1] Huang W D. Laser Solid Forming. Xi’an: Northwestern Polytechnical University Press, 2007: 16
(黄卫东. 激光立体成形. 西安: 西北工业大学出版社, 2007: 16)
[2] Liu Z X, Huang W D, Yang S. Chin J Nonferrous Met, 2002; 12: 458
(刘振侠, 黄卫东, 杨 森. 中国有色金属学报, 2002; 12: 458)
[3] Zhao Y Z, Shi Y W. Mater Rev, 2003; 17: 14
(赵玉珍, 史耀武. 材料导报, 2003; 17: 14)
[4] Dress W B, Zacharia T, Radhakrishnan B. In: Zacharia T ed., International Conference on Modeling and Control of Joining Process, AWS/ORNL Orlando, Florida, 1993: 10
[5] Grujicic M, Cao G, Figliola R S. Appl Surf Sci, 2001; 43: 57
[6] Lin X, Yang H O, Chen J, Huang W D. Acta Matell Sin, 2006; 42: 368
(林 鑫, 杨海欧, 陈 静, 黄卫东. 金属学报, 2006; 42: 368)
[7] Liu J C, Li L J. Opt Laser Technol, 2005; 37: 292
[8] Toyserkani E, Khajepour A, Corbin S. Opt Lasers Eng, 2004; 41: 867
[9] Jia W P, Chen J, Lin X, Zhong C W, Huang W D. Acta Metall Sin, 2007; 43: 552
(贾文鹏, 陈 静, 林 鑫, 钟诚文, 黄卫东. 金属学报, 2007; 43: 552)
[10] Lin X, Li Y M, Wang M, Feng L P, Chen J, Huang W D. Sci China, 2003; 33: 460
(林 鑫, 李延民, 王 猛, 冯丽萍, 陈 静, 黄卫东. 中国科学, 2003; 33: 460)
[11] Porter D A, Easterling K E. Phase Transformations in Metal and Alloys. 3rd Ed., London: Chapman and Hall, 1992: 168
[12] Poole W J , Weinberg F. Metall Mater, 1998; 29A: 861
[13] Kurz W, Fisher D J. Foundamentals of Solidification. 3rd Ed., Aedermansdorf, Switzerland, Trans Tech Publications, 1992: 233 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|