| INFLUENCE OF HEAT TREATMENT ON MICROSTRUCTURES AND ADHESIVE STRENGTH OF HIGH TEMPERATURE SOLID SELF–LUBRICANT COATING |
| XU Na 1;2; ZHANG Jia 2; HOU Wanliang 2; QUAN Mingxiu 2; LI Rongde 1; CHANG Xinchun 2 |
1. Shenyang University of Technology; Shenyang 110178
2. Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
XU Na ZHANG Jia HOU Wanliang QUAN Mingxiu LI Rongde CHANG Xinchun. INFLUENCE OF HEAT TREATMENT ON MICROSTRUCTURES AND ADHESIVE STRENGTH OF HIGH TEMPERATURE SOLID SELF–LUBRICANT COATING. Acta Metall Sin, 2009, 45(8): 943-948.
|
|
|
Abstract Foil air bearings are self–acting hydrodynamic bearings relying on solid lubricants to reduce friction and wear during sliding at start–up and shut–down when speeds are too low to allow the formation of a hydrodynamic air film. The service temperature of traditional solid lubricants such as graphite, PTFE and MoS2 is limited to only about 300 ℃, The NiCr–Cr2O3–Ag–BaF2/CaF2 solid lubricants can make foil air bearings run from room temperature to 650 ℃ In this paper, the NiCr–Cr2O3–Ag–BaF2/CaF2 high temperature solid self–lubricant coatings were fabricated on GH4169 matrix using plasma spray technology. Microstructures and adhesive strengths of the coatings as sprayed and treated at 500, 650 and 800 ℃ were analyzed by SEM, XRD and tensile test. The results show that the as–sprayed coating consists of Ni(Cr) phase, Cr2O3 phase, Ag phase and (Ba,Ca)F phase and has coarse lamellar–likstructures, the adhesive strength reaches 30.4 MPa. After heat treatments at 500 and 650 ℃ (Ba, Ca)F phase transforms into BaF2/CaF2 phase, meanwhile the BaF2/CaF2 becames compacted. The formatin and growth of lots of black Cr2Oand iO precipitations make Ni(Cr) phase refine. After heat treatment at 650 ℃ for 12 or 24 h, the adhesive strength increases to 46.5 MPa. But after heat treatment at 800 ℃ BaF2 was oxidized, which makes the microstructures loose and the porosities are formed in a large area. The adhesive strength is decreased evidently.
|
|
Received: 19 March 2009
|
|
|
| [1] Dellacorte C, Fellenstein J A, Benoy P A. Evaluation of Advanced Solid Lubricant Coatings for Foil Air Bearings Operating at 25 and 500℃, NASA TM–206619. Springfield, VA: National Technical Information Service, 1998
[2] Radil K C, Dellacorte C. The Effect of Journal Roughness and Foil Coatings on the Performance of Heavily Loaded Foil Air Bearings, NASA TM–210941. Springfield, VA: National Technical Information Service, 2001
[3] Bali´e E E, Blanchet T A. Wear, 2005; 259: 876
[4] Dellacorte C. The Evaluation of a Modified Chrome Oxide Based High Temperature Solid Lubricant Coating for Foil Gas Bearings, NASA TM–208660. Springfield, VA: National Technical Information Service, 1998
[5] Stanford M K, Dellacorte C. Friction and Wear Characteristics of Cu–4Al Foil Bearing Coating at 25 and 650 ℃, NASA TM–212972. Springfield, VA: National Technical Information Service, 2004
[6] Dellacorte C, Lukaszewicz V, Valco M J, Radil K C, Heshmat H. Performance and Durability of High Temperature Foil Air Bearings for Oil–Free Turbomachinery, NASA TM–209187. Springfield, VA: National Technical Information Service, 2000
[7] Heshmat H, Hryniewicz P, Walton II J F, Willis J P, Jahanmir S, Dellacorte C. Tribol Int, 2005; 38: 1059
[8] Fanning C E, Blanchet T A. Wear, 2008; 265: 1076
[9] Dellacorte C, Zaldana A R, Radil K C. A Systems Approach to the Solid Lubrication of Foil Air Bearings for Oil–Free Turbomachinery, NASA TM–211482. Springfield, VA: National Technical Information Service, 2002
[10] Dellacorte C. The Effects of Substrate Material and Thermal Processing Atmosphere on the Strength of PS304: A High Temperature Solid Lubricant Coating, NASA TM 211483. Springfield, VA: National Technical Information Service, 2002
[11] Stanford M K, Yanke A M, Dellacorte C. Thermal Effects on a Low Cr Modification of PS304 Solid Lubricant Coating, NASA TM–213111. Springfield, VA: National Technical Information Service, 2004
[12] Stanford M K, Dellacorte C. Effects of Humidity on the Flow Characteristics of PS304 Plasma Spray Feedstock Powder Blend, NASA TM–211549. Springfield, VA: National Technical Information Service, 2002
[13] Stanford M K, Dellacorte C, Eylon D. Particle Morphology Effects on Flow Characteristics of PS304 Plasma Spray Coating Feedstock Powder Blend, NASA TM–211206. Springfield, VA: National Technical Information Service, 2002
[14] Stanford M K, Dellacorte C, Eylon D. Particle Size Effects on Flow Properties of PS304 Plasma Spray Feedstock Powder Blend, NASA TM–211550. Springfield, VA: National Technical Information Service, 2002
[15] Stanford M K, Dellacorte C. Water Atomization of Barium Fluoride–Calcium Fluoride for Enhanced Flow Characteristics of PS304 Feed–stock Powder Blend, NASA TM–212125. Springfield, VA: National Technical Information Service, 2003
[16] Stanford M K. PhD thesis, University of Dayton, Dayton, OH, 2002
[17] Deadmore D L, Sliney H E. Hardness of CaF2 and BaF2 Solid Lubricants at 25 to 670℃, NASA TM-88979. Springfield, VA: National Technical Information Service, 1987 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|