Abstract Oscillation marks formation for slab continuous casting with high casting speed was expatiated through stress analyses of initial solidifying meniscus shell during an oscillation cycle with stabilizing casting status at 2.0 m•min-1 casting speed, and the “Extra Liquid Volume” model about position of oscillation marks formation was explained. The results show that ferrostatic pressure, friction force and flux channel pressure act on shell bring on oscillation marks along with solidification progress, and the marks position primarily lies on solidified mass fraction of solidifying shell mushy zone.
|
Received: 26 December 2006
|
|
[1]Takeuchi E,Brimacombe J K.Metall Trans,1985;16B: 605 [2]Lei Z S,Ren Z M,Zhang B W,Deng K.Acta Metall Sin, 2002;38:877 (雷作胜,任忠鸣,张邦文.邓康.金属学报,2002;38:877) [3]Schwerdtfeger K,Sha H.Metall Mater Trans,2000;31B: 813 [4]Badri A,Natarajan T T,Snyder C C,Powers K D,Man- nion F J,Byrne M,Cramb A W.Metall Mater Trans, 2005;36B:373 [5]Takeuchi E,Brimacombe J K.Metall Trans,1984;15B: 493 [6]Suzuki M,Mizukami H,Kitagawa T,Kawakami K,Uchida S,Komatsu Y.ISIJ Int,1991;31:254 [7]Zhu L G,Wang S M,Jin S T.J Univ Sci Technol Beijing, 1999;21:13 (朱立光,王硕明,金山同.北京科技大学学报,1999;21:13) [8] Meng X N,Zhu M Y,Liu X D,Cheng N L,Jiang Z K. Acta Metall Sin,2007;43:205 (孟祥宁,朱苗勇,刘旭东,程乃良,江中块.金属学报,2007;43:205) [9]Zhang J M,Zhang L,Wang X H,Wang L F.Acta Metall Sin,2003;39:1285 (张炯明,张立,王新华,王立峰.金属学报,2004;39:1285) [10]Bikerman J J.Physical Surfaces.London:Academic Press,1970:12 [11]Cramb A W,Jimbo I.Steel Res,1989;60:157 [12]Meng X N,Zhu M Y.Chin J Process Eng,2006; 6(Suppl.1):91 (孟祥宁,朱苗勇.过程工程学报,2006;6(增刊1):91) [13]Meng X N,Zhu M Y.Chin Mech Eng,in press (孟祥宁,朱苗勇.中国机械工程,待发表) [14]Szekeres E S.Iron Steel Eng,1996;73:29 [15]Meng X N,Zhu M Y.J Iron Steel Res,in press (孟祥宁,朱苗勇.钢铁研究学报,待发表) |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|