| Numerical Simulation for the Interfacial Behavior of Steel and Slag in a Slab Continuous Casting Mold with High Casting Speed |
| Na CAO |
| 东北大学材料与冶金学院 |
|
Cite this article:
Na CAO. Numerical Simulation for the Interfacial Behavior of Steel and Slag in a Slab Continuous Casting Mold with High Casting Speed. Acta Metall Sin, 2007, 43(8): 834-838 .
|
|
|
Abstract The entrainment of steel and slag interface has a great effect on casting process and the product quality. The research described the interfacial behavior between fluid steel and molten slag layer in a slab continuous casting mold with high casting speed by numerical simulation method. Good agreement between the mathematical model and experimental observation was obtained. The influences of casting speed, mold width, port angle, submergence depth of SEN and molten slag viscosity on interfacial behavior were investigated. For a given casting speed, increasing the penetration depth and downward port degree can effectively restrain interfacial oscillations. Molten slag viscosity has hardly influence on interfacial profile of steel and slag. Steel-slag interface velocity decreases with increasing molten slag viscosity.
|
|
Received: 22 December 2006
|
|
|
[1]Ilegbusi O J,Szekely J.ISIJ Int,1994;34:943 [2]Panaras G A,Theodorakakos A,Bergeles G.Metall Mater Trans,1998;29B:1117 [3]Theodorakakos A,Bergeles G.Metall Mater Trans,1998; 29B:1321 [4]Tan L J,Shen H F,Liu B C,Liu X,Xu R J,Li Y Q.Acts Metall Sin,2003;39:435 (谭利坚,沈厚发,柳百成,刘晓,徐荣军,李永全.金属学报,2003:39:435) [5]Anagnostopoulos J,Bergeles G.Metall Mater Trans, 1999;30B:1095 [6]Dash S K,Mondal S S,Ajmani S K.Int J Num Methods Heat Fluid Flow,2004;14:606 [7]Gupta D,Lahiri A K.Metall Mater Trans,1994;25B:227 [8]Lei H,Xu H H,Zhu M Y,Gan Y,Liu X,Ni M S,Liu J Q.Iron Steel,1999;34(8):20 (雷洪,许海虹,朱苗勇,干勇,刘新,倪满森,刘家奇.钢铁,1999;34(8):20) [9]Iguchi M,Yoshida J,Shimizu T,Mizuno Y.ISIJ Int,2000; 40:685 [10]Huang X,Thomas B G.Can Metall Q,1998;37:197 [11]McDavid R M,Thomas B G.Metall Mater Trans,1996; 27B:672 [12]Hirt C W,Nichols B D.J Comput Phys,1981;39:201 [13]Obbink O.PhD Dissertation,University of London,1997 [14]Brackbill J U,Kothe D B,Zemach C.J Comput Phys, 1992;100:335 [15]Launder B E,Spalding D B.Comput Method Appl Mech Eng,1974;3:269 [16]Li B Z.Refractories,2006;40:306 (李博知.耐火材料,2006;40:306)s |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|