Abstract  Effect of niobium on the microstructural and mechanical properties of as-cast Ti-48Al-0.7B cast alloy has been systematically studied in the paper. It has been found Ti-48Al-0.7B-5Nb alloy has the minimum grain size and the optimum balance mechanical properties.
Key words:  TiAl alloys      car exhaust valve      microstructure      
Received:  20 September 2006     
ZTFLH:  TG146  
  TG113.1  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I5/482

[1] Kim Y W. JOM, 1994; 46(7): 30
[2] Meier G H , Pettit F S H. Mater Sci Technol, 1992; 8: 331
[3] Sheng W B, Yang R, Liu Y Y, Xu D S, Li D. Foundry, 2001; 50: 650 (盛文斌,杨锐,刘羽寅,徐东生,李东.铸造,2001;50: 650)
[4] Liu Y, Huang B Y. Chin J Nonferrous Met, 2000; 10: 59 (刘咏,黄伯云.中国有色金属学报, 2000;10:59)
[5] Isobe S, Noda T. In: Nathal M V, ed., Structural Inter- metallics, Warrendale, PA: TMS, 1997: 427
[6] Edowlig W, Donlon W T, Allison J E. Mater Res Soc Symp Proc, 1995; 364: 757
[7] Keller M M, Jones P E, Porter W J. JOM, 1997; 49: 42
[8] Liu K, Ma Y C, Gao M, Rao G B, Li Y Y, Ke W, Wu X H, Loretto M H. Intermetallics, 2005; 13: 925
[9] Dimiduk D M. Mater Sci Eng, 1999; A263: 281
[10] Hyman M E, McCullough C, Levi C G, Mehrabian R. Metall Trans, 1991; 22A: 1647
[11] Hu D. Intermetallics, 2002; 10: 851
[12] Zhong J G. Error Theory and Datum handling. Beijing: Chemical Industry Press, 1992: 342 (钟继贵.误差理论与数据处理.北京:化学工业出版社,1992: 342)
[13] Jiang Z G, Ma Y C, Chen B, Zhao X J, Gao M, Liu K, Li Y Y. Intermetallics, in press
[14] Cheng T T. Intermetallics, 2000; 8: 29
[15] Chen G L, Zhang W J, Liu Z C, Li S J. In: Kim Y W, ed., Gamma Titanium Aluminides, Warrendale, PA: TMS, 1999: 371
[16] Chen B. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2005 (陈波.中国科学院金属研究所博士学位论文,沈阳,2005)
[17] Chen G L, Liu Z C, Lin J P, Zhang W J. In: Hemeker K J, ed., Structural Intermetallics, Warrendale, PA: TMS, 2001: 475
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[6] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[11] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[12] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[13] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[14] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[15] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
No Suggested Reading articles found!