| Effect of Excess Free Carbon on Microstructure and Strength of SiC Fiber |
| Changyou Guo |
| 东北大学理学院 |
|
Cite this article:
Changyou Guo. Effect of Excess Free Carbon on Microstructure and Strength of SiC Fiber. Acta Metall Sin, 2007, 43(2): 165-170 .
|
|
|
Abstract Analytical electron microscope (AEM) was applied to investigate the effect of excess free carbon on the microstructure of SiC fiber during SiC deposition growth and relation between microstructure and strength of SiC fiber. The results indicate excess free carbon addition can make effects on microstructure in two aspects. One is that carbon addition can effectively avoid WO3 formation at W/SiC interface, and then, as a result, get rid of oxygen element in fiber; the other is that it can reduce grain size of SiC, especially adjacent to W core. In addition, many concentric C rich layers form within inner SiC sheath. Above changes in microstructure play a positive role in improving fiber’s strength
Key words: SiC fiber, analytical electron microscope (AEM), microstructure, strength.
|
|
Received: 21 July 2006
|
|
|
[1]Dicarlo J A.J Met,1985;37(6):44 [2]Hooker J A,Doorbar P J.Mater Sci Technol,2000;16:725 [3]Guo Z X,Derby B.Prog Mater Sci,1995;39:411 [4]Wang S Y,Zhang R G.Fibers Reinforced Composites,Shanghai:Donghua University Press,1998(王善元,张汝光.纤维增强复合材料,上海:东华大学出版社,1998) [5]Leyen C,Hausmann J,Kumpfert J.Adv Eng Mater,2003;5:399 [6]Cheng TT,Jones I P,Shatwell R A,Doorbar P.MaterSci Eng,1999;A260:139 [7]Wawner F W,Teng A Y,Nutt S R.SAMPE Q,1983;14(3):39 [8]Ning X J,Pirouz P.J Mater Res,1991;6(10):2234 [9]Shinozaki S S,Sato H.J Am Ceram Soc,1978;61:425 [10]Keyse R J,Garratt-Reed A J,Goodhew P J,Lorimer G W.Introduction to Scanning Transmission Electron Microscopy,Singapore:Springer,1998 [11]Guo C Y,Zhang C B,He L L,Jin B H,Shi N L.J Mater Sci Technol,accepted [12]Smith P R,Froes F H.J Met,1984;(March):19 [13]Fred G,Rainer S F.Mater Sci Eng,1995;B34:224 [14]Deng J,Luo G Z,Ding W Z.Rare Met Mater Eng,1991;20(6):10(邓炬,罗国珍,丁文周.稀有金属材料与工程,1991;20(6):10) [15]Dyos K,Shatwell R A.J Microsc,1999;196:175 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|