| MICROSTRUCTURE SIMULATION OF Al-Si/SiCp COMPOSITES WITH PARTICLE PUSHING MODEL |
| LI Bin; XU Qingyan; LI Xudong; LIU Baicheng |
| Key Laboratory for Advanced Manufacturing by Materials Processing Technology; Department of Mechanical Engineering; Tsinghua University; Beijing 100084 |
|
Cite this article:
LI Bin; XU Qingyan; LI Xudong; LIU Baicheng. MICROSTRUCTURE SIMULATION OF Al-Si/SiCp COMPOSITES WITH PARTICLE PUSHING MODEL. Acta Metall Sin, 2005, 41(12): 1303-1308 .
|
|
|
Abstract The microstructure of SiC particle reinforced Al-7.0%Si (mass
fraction) composite prepared by stir casting was simulated by
a modified cellular automaton method coupled with finite difference
method and two-dimensional models under normal solidification
condition including macro heat transfer, nucleation, equiaxed dendrite
growth and particle pushing. The effects of different casting
processes on composite microstructure and particle distribution were
analyzed. The simulated results can clearly show the evolution of the
microstructure of composite and particle clustering phenomena caused by
particle pushing. The simulated results are in good agreement
with the experimental results. Grain size is smaller and particle
distribution is more uniform for metal mould casting than sand mould casting.
|
|
Received: 14 April 2005
|
|
|
[1] Jung C K, Jung S W, Nam H W, Han K S. J Compos Mater, 2003; 37: 503 [2] Yang N, Boselli J, Gregson P J, Sinclair I. Mater Sci Tech- nol, 2000; 16: 797 [3] Kang C G, Ray S, Rohatgi P K. Mater Sci Eng, 1994; A188: 193 [4] Wang C Y, Beckermann C. Metall Mater Trans, 1996; 27 A: 2754 [5] Feller R J, Beckermann C. Metall Mater Trans, 1997; 28B: 1165 [6] Kim J K, Rohatgi P K. Acta Mater, 1998; 46: 1115 [7] Juretzko F R, Dhindaw B K, Stefanescu D M, Sen S, Cur- reri P A. Metall Mater Trans, 1998; 29A: 1691 [8] Stefanescu D M, Juretzko F R, Dhindaw B K, Catalina A, Sen S, Curreri P A. Metall Mater Trans, 1998; 29A: 1697 [9] Catalina A V, Mukherjee S, Stefanescu D M. Metall Mater Trans, 2000; 31A: 2559 [10] Shangguan D K, Ahuja S, Stefanescu D M. Metall Trans, 1992; 23A: 669 [11] Stefanescu D M. Key Eng Mater, 1993; 79-80: 74 [12] Hu H Q. Principles of Metal Solidification. Beijing: China Machine Press, 2000 (胡汉起.金属凝固原理.北京:机械工业出版社, 2000) [13] Kurz W, Giovanola B, Trivedi R. Ada Metall, 1986; 34: 823 [14] Pan Y H. Computer Graphics: Principles, Methods and Applications. Beijing: Higher Education Press, 2001 (潘云鹤.计算机图形学:原理、方法及应用.北京:高等教育 出版社,2001) [15] Xu Q Y, Feng W M, Liu B C, Xiong S M. Acta Metall Sin, 2002; 38: 799 (许庆彦,冯伟明,柳百成,熊守美.金属学报,2002;38:799) [16] Feng W M, Xu Q Y, Liu B C. ISIJ Int, 2002; 42: 702 [17] Garvin J W, Udaykumar H S. J Cryst Growth, 2003; 252: 451 [18] Stefanescu D M, Dhindaw B K, Kacar S A, Moitra A. Metall Trans, 1988; 19A: 2847 [19] Feng W M. Master Degree Thesis, Tsinghua University, Beijing, 2002 (冯伟明.清华大学硕士学位论文,北京, 2002) |