Abstract Using spark plasma sintering technique, a bulk Al90Mn9Ce1
alloy, reinforced by quasicrystal particles, has been sintered under the
pressure of 50 MPa at 400 ℃. The density and the compressive strength of
the as-prepared bulk alloy are above 98% and 1000 MPa, respectively.
It has been found that during the spark plasma sintering process, under
the condition of large current, short sintering time and lower sintering
temperature, the metastable icosahedron quasicrystal phase in primary
powder particles is kept. And the strong discharge plasma among particles
can decompose or break the oxide film on the primary powder's surface,
resulting in the increment of their combination strength. So the
as-prepared bulk alloy possesses high density and ultra-high strength.
|
|
Received: 01 July 2005
|
|
|
[1] Inoue A. Prog Mater Sci, 1998; 43: 365 [2] Inoue A. Ada Mater, 2000; 48: 279 [3] Schurack F, Bckert J, Schultz L. Acta Mater, 2001; 49: 1351 [4] Zhao Z K, Li J C, Jiang Q. J Mater Eng Perform, 2002; 11: 262 [5] Zhao Z K, Yao K F, Li J C, Jiang Q. Acta Metll Sin, 2004; 40: 355 (赵占奎,姚可夫,李建忱,蒋青.金属学报,2004;40:355) [6] Mamedov V. Powd Metall, 2002; 45: 322 [7] Wen C E, Mabuchi M, Yamada Y, Shimojima K, Chino Y, Hosokawa H, Asahina I. J Mater Sci Lett, 2003; 22: 1407 [8] Luo Y M, Li S Q, Wei P, Liu L. Mater Lett, 2004; 58: 150 [9] Thostenson E T, Ren Z F, Chou T W. Comp Sci Technol, 2001; 61: 1899 [10] Liu W P, Naka M. Scr Mater, 2003; 48: 1225 [11] Shen B L, Kimura H, Inoue A, Omori M, Okubo A. Mater Trans, 2002; 43: 1961 [12] Xie G Q, Ohashi O, Yamaguchi N, Wang A R. Metall Mater Trans, 2003; 34A: 2655 [13] Inoue A, Watanabe M, Kimura H M, Takehashi F, Nagata A, Masumoto T. Mater Trans JIM, 1992; 33: 723 [14] Shechtman D, Blech I. Metall Trans, 1985; 16A: 10p |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|