The influence of size effect of conductivity on the microwave absorption properties of thin Al films
terry liau;Hao Du;;;;Li-shi WEN
中科院金属所
Cite this article: 

terry liau; Hao Du; Li-shi WEN. The influence of size effect of conductivity on the microwave absorption properties of thin Al films. Acta Metall Sin, 2008, 44(9): 1099-1104 .

Download:  PDF(1850KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Thin Aluminum films with different thickness were deposited on PET substrate by Mid-frequency Magnetron Sputtering (MFMS). The DC conductivity of these thin films was measured using linear four probe method. The microwave absorption properties of the Al-FR4 epoxy layered structure were characterized by vector network analyzer. The results indicated that the size effect on conductivity have a pronounced influence on microwave absorption properties of the thin aluminum film, which were verified by theoretical calculation with transfer matrix method.
Key words:  aluminum films      size effect      microwave absorption      transfer matrix method      
Received:  17 December 2007     
ZTFLH:  O484.5  
  TB43  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I9/1099

[1]Born M,Wolf E.Principles of Optics.Oxford:Pergamon Press,1983:612
[2]Kong J A.Electromagnetic Wave Theory.Cambridge, MA:EMW Publishing,2005:181
[3]Bosman H L,Lau Y Y,Gilgenbach R M.Appl Phys Lett, 2003;82:1353
[4]Bosman H L,Lau Y Y,Gilgenbach R M.IEEE Trans Plasma Sci,2004;32:1292
[5]Chambers B,Tennant A.Electron Lett,1994;30:1797
[6]Chambers B.Electron Lett,1994;30:1626
[7]Eriksson A,Deleniv A,Gevorgian S.2002 IEEE MTTS International Microwave Symposium Digest,Vol.3,Seat- tle,WA,MTT-S,2002:2009
[8]Fuchs K.Proc Cambridge Philas Soc,1938;34:100
[9]Sondheimer E H.Adv Phys,1952;1:1
[10]Softer S B.J Appl Phys,1967;38:1710
[11]Namba Y.Jpn J Appl Phys,1970;9:1326
[12]Govindaxaj G,Devanathan V.Phys Rev,1986;34B:5904
[13]Trivedi N,Ashcroft N W.Phys Rev,1988;38B:12298
[14]Makarov N M,Moroz A V,Yampolskii V A.Phys Rev, 1995;52B:6087
[15]Ashcroft N W,Mermin N D.Solid State Physics.New York:Brooks/Cole,1976:350
[16]Mayadas A F,Shatzkes M,Janak J F.Phys Rev,1970; 1B:1382
[17]Pozar D M.Microwave Engineering.3rd ed.,New York: Wiley,2005:51
[18]Lee M-H J,Collier R J.Microelectron Eng,2004;73-74: 916
[19]Kittel C.Introduction to Solid State Physics.New York: Wiley,2004:213
[20]Ramo S,Whinnery J R,Duzer T V.Fields and Waves in Communication Electronics.3rd ed.,New York:Wiley, 1994:290
[21]Shavit R,Smolski A P,Michielssen E,Mitta R.IEEE Trans Antennas Propag,1992;40:126
[22]Misran N,Cahill R,Fusco V F.Electron Lett,2003;39: 1628
[23]Frenkel A.Electron Lett,2001;37:1374
[24]Matsumoto M,Miyata Y.IEEE Trans Magn,1997;33: 4459
[1] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[2] YU Shaoxia, WANG Qi, DENG Xiangtao, WANG Zhaodong. Preparation and Size Effect of GH3600 Nickel-Based Superalloy Ultra-Thin Strips[J]. 金属学报, 2023, 59(10): 1365-1375.
[3] CAO Qingping, LV Linbo, WANG Xiaodong, JIANG Jianzhong. Magnetron Sputtering Metal Glass Film Preparation and the “Specimen Size Effect” of the Mechanical Property[J]. 金属学报, 2021, 57(4): 473-490.
[4] QU Ruitao, WANG Xiaodi, WU Shaojie, ZHANG Zhefeng. Research Progress in Shear Banding Deformation and Fracture Mechanisms of Metallic Glasses[J]. 金属学报, 2021, 57(4): 453-472.
[5] Guangping ZHANG, Honglei CHEN, Xuemei LUO, Bin ZHANG. Progress in Thermal Fatigue of Micro/Nano-ScaleMetal Conductors[J]. 金属学报, 2018, 54(3): 357-366.
[6] Yefei MA, Zhuman SONG, Siqian ZHANG, Lijia CHEN, Guangping ZHANG. Evaluation of Fatigue Properties of CA6NM Martensite Stainless Steel Using Miniature Specimens[J]. 金属学报, 2018, 54(10): 1359-1367.
[7] Rui YANG,Yan PAN,Wei CHEN,Qiaoyan SUN,Lin XIAO,Jun SUN. DEFORMATION BEHAVIOR AND THE MECHANISM OF MICRO-SCALE Ti-10V-2Fe-3Al PILLARSIN COMPRESSION[J]. 金属学报, 2016, 52(2): 135-142.
[8] Jun SUN, Jinyu ZHANG, Kai WU, Gang LIU. SIZE EFFECTS ON THE DEFORMATION AND DAMAGEOF Cu-BASED METALLIC NANOLAYEREDMICRO-PILLARS[J]. 金属学报, 2016, 52(10): 1249-1258.
[9] LIU Yuan, LIU Xiangxuan, WANG Xuanjun, CHEN Xin. Fe THIN FILMS GROWN ON SURFACE OF SrFe12O19 BY MOCVD METHOD AND ITS ABSORBING PROPERTIES[J]. 金属学报, 2014, 50(9): 1095-1101.
[10] HUANG Xiaoxu. SIZE EFFECTS ON THE STRENGTH OF METALS[J]. 金属学报, 2014, 50(2): 137-140.
[11] ZHANG Jinyu, LIU Gang, SUN Jun. SIZE EFFECTS ON DEFORMATION AND FRACTURE BEHAVIOR OF NANOSTRUCTURED METALLIC MULTILAYERS[J]. 金属学报, 2014, 50(2): 169-182.
[12] DENG Liping, YANG Xiaofang, HAN Ke, SUN Zeyuan, LIU Qing. STUDY ON THE MICROSTRUCTURE EVOLUTION OF Cu-Nb COMPOSITE WIRES DURING DEFORMATION AND ANNEALING[J]. 金属学报, 2014, 50(2): 231-237.
[13] ZHANG Jinyu ZHANG Xin NIU Jiajia LIU Gang ZHANG Guojun SUN Jun. LENGTH SCALE DEPENDENT MECHANICAL/ELECTRICAL PROPERTIES OF Cu/X (X=Cr, Nb) NANOSTRUCTURED METALLIC MULTILAYERS[J]. 金属学报, 2011, 47(10): 1348-1354.
[14] YIN Limeng YANG Yan LIU Liangqi ZHANG Xinping. SIZE EFFECT OF MECHANICAL BEHAVIOR OF MINIATURE SOLDER JOINT INTERCONNECTIONS IN ELECTRONIC PACKAGING[J]. 金属学报, 2009, 45(4): 422-427.
[15] XU Ze-Jian. MICROHARDNESS INVESTIGATION OF 0Cr18Ni10Ti STAINLESS STEEL WELDED JOINT[J]. 金属学报, 2008, 44(5): 636-640 .
No Suggested Reading articles found!