| The influence of size effect of conductivity on the microwave absorption properties of thin Al films |
| terry liau;Hao Du;;;;Li-shi WEN |
| 中科院金属所 |
|
Cite this article:
terry liau; Hao Du; Li-shi WEN. The influence of size effect of conductivity on the microwave absorption properties of thin Al films. Acta Metall Sin, 2008, 44(9): 1099-1104 .
|
|
|
Abstract Thin Aluminum films with different thickness were deposited on PET substrate by Mid-frequency Magnetron Sputtering (MFMS). The DC conductivity of these thin films was measured using linear four probe method. The microwave absorption properties of the Al-FR4 epoxy layered structure were characterized by vector network analyzer. The results indicated that the size effect on conductivity have a pronounced influence on microwave absorption properties of the thin aluminum film, which were verified by theoretical calculation with transfer matrix method.
|
|
Received: 17 December 2007
|
|
|
[1]Born M,Wolf E.Principles of Optics.Oxford:Pergamon Press,1983:612 [2]Kong J A.Electromagnetic Wave Theory.Cambridge, MA:EMW Publishing,2005:181 [3]Bosman H L,Lau Y Y,Gilgenbach R M.Appl Phys Lett, 2003;82:1353 [4]Bosman H L,Lau Y Y,Gilgenbach R M.IEEE Trans Plasma Sci,2004;32:1292 [5]Chambers B,Tennant A.Electron Lett,1994;30:1797 [6]Chambers B.Electron Lett,1994;30:1626 [7]Eriksson A,Deleniv A,Gevorgian S.2002 IEEE MTTS International Microwave Symposium Digest,Vol.3,Seat- tle,WA,MTT-S,2002:2009 [8]Fuchs K.Proc Cambridge Philas Soc,1938;34:100 [9]Sondheimer E H.Adv Phys,1952;1:1 [10]Softer S B.J Appl Phys,1967;38:1710 [11]Namba Y.Jpn J Appl Phys,1970;9:1326 [12]Govindaxaj G,Devanathan V.Phys Rev,1986;34B:5904 [13]Trivedi N,Ashcroft N W.Phys Rev,1988;38B:12298 [14]Makarov N M,Moroz A V,Yampolskii V A.Phys Rev, 1995;52B:6087 [15]Ashcroft N W,Mermin N D.Solid State Physics.New York:Brooks/Cole,1976:350 [16]Mayadas A F,Shatzkes M,Janak J F.Phys Rev,1970; 1B:1382 [17]Pozar D M.Microwave Engineering.3rd ed.,New York: Wiley,2005:51 [18]Lee M-H J,Collier R J.Microelectron Eng,2004;73-74: 916 [19]Kittel C.Introduction to Solid State Physics.New York: Wiley,2004:213 [20]Ramo S,Whinnery J R,Duzer T V.Fields and Waves in Communication Electronics.3rd ed.,New York:Wiley, 1994:290 [21]Shavit R,Smolski A P,Michielssen E,Mitta R.IEEE Trans Antennas Propag,1992;40:126 [22]Misran N,Cahill R,Fusco V F.Electron Lett,2003;39: 1628 [23]Frenkel A.Electron Lett,2001;37:1374 [24]Matsumoto M,Miyata Y.IEEE Trans Magn,1997;33: 4459 |
| No Suggested Reading articles found! |
|
|