EFFECTS OF GRAIN-BOUNDARY PHASES ON HYDROGEN EMBRITTLEMENT OF FE-NI-CR AUSTENITIC ALLOY BY INTERNAL FRICTION
Jian ZHANG;;;
中国科学院金属研究所特殊环境材料研究部
Cite this article:
Jian ZHANG. EFFECTS OF GRAIN-BOUNDARY PHASES ON HYDROGEN EMBRITTLEMENT OF FE-NI-CR AUSTENITIC ALLOY BY INTERNAL FRICTION. Acta Metall Sin, 2008, 44(9): 1095-1098 .
Abstract Dynamic mechanical analyzer (DMA) was used to investigate the hydrogen embrittlement of two Fe-Ni-Cr austenitic alloys. The effects of hydrogen and grain-boundary phases on internal friction of the alloys were analyzed. Optical microscopy and scanning electron microscopy were used to observe the microstructures and grain-boundary phases. The results show that abundant Ni3Ti phases and little carbides precipitated at grain boundaries in the alloy without boron, while and only little Ni3Ti phase and carbides precipitated at grain boundaries in the alloy with boron. Thermal hydrogen charging caused two new internal friction peaks at about 27℃ and 36℃ in the alloys with and without boron respectively, and the peaks were resulted from the interaction between hydrogen atoms and the interfaces of grain-boundary phases. Boron decreased the temperature of hydrogen-induced internal friction peaks, indicating that the diminishing in grain-boundary phase by boron reduced the ability of grain boundary to trap hydrogen atoms. As a result, boron lowered the ductility loss of the alloy.
[1]Thompson A W.Mater Sci Eng,1974;14:253 [2]Louthan M R,Caskey G R,Donovan J A,Rawl D E.Mater Sci Eng,1972;10:357 [3]Ma L M,Liang G J,Fan C G,Li Y Y.Acta Metall Sin (Engl Lett),1997;10:206 [4]Ma L M,Li Y Y,Liu S W,Chen L.Acta Metall Sin,1988; 24:B427 (马禄铭,李依依,刘树望,陈廉.金属学报,1988;24:B427) [5]Zhang J,Li X Y,Rong L J,Zheng Y N,Zhu S Y.Acta Metall Sin,2006;42:469 (张建,李秀艳,戎利建,郑永男,朱升云.金属学报,2006;42:469) [6]Asano S,Shibata M,Tsunoda R.Scr Metall,1980;14: 377 [7]McLellan R B,Yoshihara M.Acta Metall,1987;35:197 [8]West A J,Louthan M R.Metall Trans,1979;10A:1675 [9]Gavriljuk V G,Hanninen H,Jagodzinsky Y N,Tarasenko A V,Tahtinen S,Ullakko K.Scr Metall Mater,1993;28: 901 [10]Usui M,Asano S.Scr Mater,1996;34:1691 [11]Peterson J A,Gibala R,Troiano A R.J Iron Steel Inst, 1969;207:86 [12]Xu J,Sun X K,Chen W X,Li Y Y.Acta Metall Mater, 1993;41:1455 [13]Chu W Y.Hydrogen Damage and Delayed Fracture.Bei- jing:Metallurgical Industry Press,1988:38 (褚武扬.氢损伤和滞后断裂.北京:冶金工业出版社,1988:38) [14]Messmer R P,Briant C L.Hydrogen Degradation of Fer- rous Alloys.Park Ridge,N J:Noyes Publication,1985: 140 [15]Li X Y,Rong L J,Li Y Y.Acta Metall Sin,2005;41:1155 (李秀艳,戎利建,李依依.金属学报,2005;41:1155) [16]Brooks J A,Thompson A W.Metall Trans,1993;24A: 1983