SONG Hongwei; SHI Bi; WANG Xiufang; ZHANG Junbao. Characterization of a low carbon low alloy steel by nanoindentation. Acta Metall Sin, 2005, 41(3): 287-290 .
Abstract A low carbon low alloy steel with two different types of
microstructures was characterized
by nanoindentation. The results indicate that the average
nanoindentation hardness of martensite is at least
70\% higher than that of ferrite in the dual-phase sample. Since the
ultrafine martensite grain is embedded in
the soft ferrite matrix, the nanoindentation hardness of martensite
exhibits a substrate-effect when the
indentation depth is over 40 nm. Due to more carbon
atoms partitioning to austenite during intercritical
process, carbon content of martensite in the dual-phase
sample may be several times higher than the
nominal carbon content of the steel, which makes the
average nanoindentation hardness of martensite in the
dual-phase sample is at least 30% higher than that in
the fully martensitic sample. In addition, the possible effects of
carbon partitioning on Poisson ratio and Young's
modulus of martensite were discused briefly.
[1] Oliver W C, Pharr G M. J Mater Res, 1992; 7: 1564 [2] Oliver W C, Pharr G M. J Mater Res, 2004; 19: 3 [3] Jacq C, Lormand G, Nelias D, Girodin D, Vincent A. Mater Sci Eng, 2003; A342: 311 [4] Ohmura T, Hara T, Tsuzaki K. Scr Mater, 2003; 49: 1157 [5] Randall N X, Julia-Schmutz C, Soro J M, Zacharie G. Thin Solid Films, 1997; 308-309: 297 [6] Choi Y, Choo W Y, Kwon D. Scr Mater, 2001; 45: 1401 [7] Furnemont Q, Kempf M, Jacques P J, Goken M, Delannay F. Mater Sci Eng, 2002; A328: 26 [8] Makinson J D, Weins W N, Xu Y, de Angelis R J, Ferber M K, Riester L, Lawrence R V. In: Inove K, ed., Proc 1996 Int Conf on Displacive Phase Transformations and Their Applications in Materials Engineering, Urban, Ill, USA: TMS, 1998: 391m