Acta Metall Sin  2015, Vol. 51 Issue (8): 957-966    DOI: 10.11900/0412.1961.2014.00703
Current Issue | Archive | Adv Search |
MICROSTRUCTURE EVOLUTION AND SOLUTE SEGREGATION IN DIRECTIONALLY SOLIDIFIED TiAl ALLOYS WITH HIGH Nb CONTENT
Yong LI1,Guohuai LIU1,Zhaodong WANG1,Tianliang FU1,Xinzhong LI2,Yanqing SU2,Jingjie GUO2,Hengzhi FU2
1 State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819
2 School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001
Cite this article: 

Yong LI,Guohuai LIU,Zhaodong WANG,Tianliang FU,Xinzhong LI,Yanqing SU,Jingjie GUO,Hengzhi FU. MICROSTRUCTURE EVOLUTION AND SOLUTE SEGREGATION IN DIRECTIONALLY SOLIDIFIED TiAl ALLOYS WITH HIGH Nb CONTENT. Acta Metall Sin, 2015, 51(8): 957-966.

Download:  HTML  PDF(10575KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

TiAl-Nb alloys have been determined as the advanced direction for the development of the high temperature TiAl alloys, so being one of the advanced materials for turbines of aircraft engines and gas-burning power-generation plants. However, highly-Nb addition can lead to the complex solidification behavior of TiAl-Nb alloy and multi-phase microstructure, which is important for the mechanical properties during the alloy design. Bridgman type directional solidification experiments were conducted for Ti-46Al-(8, 9, 10)Nb alloy. The effect of the growth rate and Nb content on the microstructure, phase transition and microsegregation was investigated, and finally the selection diagram of the phase transition and the microstructure of the directional solidified TiAl-Nb alloy were obtained. The results show that the planar-cellular-dendritic evolution of solid-liquid interface can be observed with the increase of the growth rate. Meanwhile the fully b phase solidification changes to the peritectic solidification with the increase of the growth rate, and correspondingly the final microstructure is composed of the a2/g lamellar structure and a multiphase microstructure (B2 phase, a2/g lamellar structure) respectively. The increase of the b-stabilizer Nb content can promote the fully b phase solidification and the formation of the multiphase microstructure (B2 phase, a2/g lamellar structure). The contribution of the growth rate and the Nb content to the phase transition and the microstructure is connected with the solute segregation (S-segregation, b-segregation) closely. The increase of the S-segregation amplitude can easily promote the peritectic reaction, which always leads to the highly solute segregation and the concentrated distribution of plenty of B2 phase in the core of the dendrite. b-segregation is the mainly origin of the B2 phase formation, in which the Nb enrichment in the retained b phase directly determines the morphology and the dimension of the B2 phase. Finally according to the selection diagram of the solidification process and the microstructure of the Ti-46Al alloy with the growth rate and the Nb content, the high Nb content and the low growth rate during fully b solidification should be selected for the prefer microstructure with the homogeneous distribution and the low solute segregation.

Key words:  TiAl-Nb alloy      directional solidification      microstructure      solute segregation     
Fund: Supported by National Natural Science Foundation of China (Nos.51071062, 51274077 and 51271068), Fundamental Research Funds for the Central Universities (No.N140703003) and China Postdoctoral Science Foundation (No.2014M561245)

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2014.00703     OR     https://www.ams.org.cn/EN/Y2015/V51/I8/957

Fig.1  Solid/liquid interface morphologies with 8%Nb (a1~e1), 9%Nb (a2~e2), 10%Nb (a3~e3) and growth rates V of 2 μm/s (a1~a3), 3 μm/s (b1~b3), 10 μm/s (c1~c3), 15 μm/s (d1~d3), 70 μm/s (e1~e3) in directional solidified Ti-46Al alloy
Fig.2  Microstructure (a), XRD spectrum (b) and the characteristics of B2 phase distribution (c, d) in directionally solidified Ti-46Al-Nb alloy (Inset in Fig.2c shows SAED pattern of B2 phase)
Phase Ti Al Nb
g 42.23 49.62 8.15
a2 47.61 44.75 7.64
B2 42.23 42.34 15.43
Table 1  Chemical compositions of the different phases in directionally solidified Ti-46Al-8Nb alloy (atomic fraction / %)
Fig.3  Longitudinal macrostructures and corresponding microstructures of directionally solidified Ti-46Al-Nb alloy with different Nb contents and growth rates

(a) macrostructure of Ti-46Al-8Nb alloy, V=2 μm/s

(b~d) microstructures of Ti-46Al-8Nb alloy, V=2 μm/s

(e) macrostructure of Ti-46Al-8Nb alloy, V=3 μm/s

(f~h) microstructures of Ti-46Al-8Nb alloy, V=3 μm/s

(i) macrostructure of Ti-46Al-10Nb alloy, V=30 μm/s

(j~l) microstructures of Ti-46Al-10Nb alloy, V=30 μm/s, inset in Fig.3l show the locally magnified image

Fig.4  Solute segregations (a1~c1) and line scan EDS along the black line (a2~c2) during the different phase transition processes of directionally solidified Ti-46Al-8Nb alloy in L+b region (a1, a2), L+b+a region (b1, b2) and a2/g+B2 region (c1, c2)
Fig.5  Solute segregation and microstructure evolution during the phase transition process of L→L+b→L+b+a (a1~c1) and L→L+b→b+a (a2~c2) in directionally solidified Ti-46Al-Nb alloy at V=5 μm/s
Fig.6  Selection diagram of the phase transition and the final microstructure with the evolution of the Nb content and the growth rate in directionally solidified Ti-46Al-Nb alloy
[1] Loria E A. Intermetallics, 2000; 8: 1339
[2] Luo W Z, Shen J, Li Q L, Man W W, Fu H Z. Acta Metall Sin, 2007; 43: 897 (罗文忠, 沈 军, 李庆林, 满伟伟, 傅恒志. 金属学报, 2007; 43: 897)
[3] Dimiduk D M. Mater Sci Eng, 1999; A263: 281
[4] Chen Y Y, Kong F T. Acta Metall Sin, 2008; 44: 551 (陈玉勇, 孔凡涛. 金属学报, 2008; 44: 551)
[5] Li X Z, Fan J L, Su Y Q, Liu D M, Guo J J, Fu H Z. Intermetallics, 2012; 27: 38
[6] Wu X. Intermetallics, 2006; 14: 1114
[7] Li H Z, Li Z, Zhang W, Wang Y, Liu Y, Wang H J. J Alloys Compd, 2010; 508: 359
[8] Wang Y H, Lin J P, He Y H, Wang Y L, Chen G L. J Alloys Compd, 2008; 456: 297
[9] Chen G L, Wang X T, Ni K Q, Hao S M, Cao J X, Zhang X. Intermetallics, 1996; 4: 13
[10] Chen G L, Sun Z Q, Zhou X. Corros Sci, 1992; 11: 939
[11] Nakamura H, Takeyama M, Yamabe Y, Kikuchi M. Scr Mater, 1993; 28: 997
[12] Leonard K J, Vasudevan V K. Intermetallics, 2000; 8: 1257
[13] Chen G L, Zhang W J, Liu Z C, Li S J, Kim Y W. Gamma Titanium Aluminizes 1999. Lerotto: TMS, 1999: 371
[14] Liu G H, Li X Z, Su Y Q, Liu D M, Guo J J, Fu H Z. J Alloys Compd, 2012; 541: 275
[15] Chen G L, Xu X J, Teng Z K, Wang Y L, Lin J P. Intermetallics, 2007; 15: 625
[16] Ding X F, Lin J P, Zhang L Q, Wang H L, Hao G J, Chen G L. J Alloys Compd, 2010; 506: 115
[17] Perdrix F, Trichrt M F, Bonnentien J L, Cornet M, Bigot J. Intermetallics, 1999; 7: 1323
[18] Ding X F, Lin J P, Zhang L Q, Song X P, Chen G L. Mater Des, 2011; 32: 395
[19] Clemens H, Kestler H. Adv Eng Mater, 2000; 2: 551
[20] Imayev R M, Imayev V M, Oehring M. Intermetallics, 2007; 15: 451
[21] Niu H Z, Chen Y Y, Xiao S L, Xu L J. Intermetallics, 2012; 31: 225
[22] Yu R, He L L, Cheng Z Y, Zhu J, Ye H Q. Intermetallics, 2002; 10: 661
[23] Trivedi R. J Cryst Growth, 1980; 49: 219
[24] Kerr H W, Cisse J, Bolling G F. Acta Metall, 1974; 22: 677
[25] Kim M C, Oh M H, Lee J H, Inui H, Yamaguchi M, Wee D M. Mater Sci Eng, 1997; A239-240: 570
[1] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[6] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[9] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[10] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[11] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[14] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[15] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
No Suggested Reading articles found!