| STUDY OF SOLIDIFICATION FOR GAS-ATOMIZED DROPLET OF Cu-Co-Fe ALLOY |
Lei ZHAO1,2,Hongxiang JIANG2,Tauseef AHMAD2,Jiuzhou ZHAO2( ) |
1 School of Mechanical Engineering, Liaoning Shihua University, Fushun 113001 2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
|
Cite this article:
Lei ZHAO,Hongxiang JIANG,Tauseef AHMAD,Jiuzhou ZHAO. STUDY OF SOLIDIFICATION FOR GAS-ATOMIZED DROPLET OF Cu-Co-Fe ALLOY. Acta Metall Sin, 2015, 51(7): 883-888.
|
|
|
|
|
|
| Fund: Supported by National Natural Science Foundation of China (Nos.51271185, 51031003 and 51471173) |
| [1] | Song J S, Hong S I. J Alloys Compd, 2000; 311: 265 | | [2] | Berkowitz A E, Mitchell J R, Carey M J, Young A P, Zhang S, Spada F E, Parker F T, Hutten A, Thomas G. Phys Rev Lett, 1992; 68: 3745 | | [3] | Dai F P, Cao C D, Wei B B. Chin Sci Bull, 2009; 54: 402 (代富平, 曹崇德, 魏炳波. 科学通报, 2009; 54: 402) | | [4] | He J, Zhao J Z. Acta Metall Sin, 2005; 41: 407 (何 杰, 赵九洲. 金属学报, 2005; 41: 407) | | [5] | Kim D I, Abbaschian R. J Phase Equilib, 2000; 21: 25 | | [6] | Cao C D, G?rler G P. Chin Phys Lett, 2005; 22: 482 | | [7] | Curiotto S, Battezzati L, Johnson E, Palumbo M, Pryds N. J Mater Sci, 2008; 43: 3253 | | [8] | Munitz A, Bamberger A M, Wannaparhun S, Abbaschian R. J Mater Sci, 2006; 41: 2749 | | [9] | Turchanin M A, Dreval L A, Abdulov A R, Agraval P G. Powder Metall Met Ceram, 2011; 50: 98 | | [10] | Bamberger M, Munitz A, Kaufman L, Abbaschian R. Calphad, 2002; 26: 375 | | [11] | Wang C P, Liu X J, Ohnuma I, Kainuma R, Ishida K. J Phase Equilib, 2002; 23: 236 | | [12] | Palumbo M, Curiotto S, Battezzati L. Calphad, 2006; 30: 171 | | [13] | Munitz A, Abbaschian R. J Mater Sci, 1998; 33: 3639 | | [14] | Dai F P, Cao C D, Wei B B. Sci Chin, 2007; 37G: 376 (代富平, 曹崇德, 魏炳波. 中国科学, 2007; 37G: 376) | | [15] | Zhou F M, Sun D K, Zhu M F. Acta Phys Sin, 2010; 59: 3394 (周丰茂, 孙东科, 朱鸣芳. 物理学报, 2010; 59: 3394) | | [16] | Cui H B, Guo J J, Su Y Q, Wu S P, Li X Z, Fu H Z. Acta Metall Sin, 2007; 43: 907 (崔红保, 郭景杰, 苏彦庆, 吴士平, 李新中, 傅恒志. 金属学报, 2007; 43: 907) | | [17] | Ranz W E, Marshall W R. Chem Eng Prog, 1952; 48: 141 | | [18] | Grant P S, Cantor B, Katgerman L. Acta Metall Mater, 1993; 41: 3097 | | [19] | Zhao L, Zhao J Z. J Mater Res, 2013; 28: 1203 | | [20] | Granasy L, Ratke L. Scr Metall Mater, 1993; 28: 1329 | | [21] | Zhao J Z. Mater Sci Eng, 2007; A454-455: 637 | | [22] | Dinsdale A T. Calphad, 1991; 15: 317 | | [23] | Turchanin M A, Agraval P G. Powder Metall Met Ceram, 2007; 46: 77 | | [24] | Turchanin M A, Agraval P G, Nikolaenko I V. J Phase Equilib, 2003; 24: 307 | | [25] | Ohnuma I, Enoki H, Ikeda O, Kainuma R, Ohtani H, Sundman B, Ishida K. Acta Mater, 2002; 50: 379 | | [26] | Moldover M R. Phys Rev, 1985; 31A: 1022 | | [27] | Brandes E A, Brook G B. Smithells Metals Reference Book. 7th Ed., Oxford: Butterworth-Heinemann Ltd, 1992: 14 | | [28] | Roy A K. Chhabra R P. Metall Trans, 1988; 19A: 273 | | [29] | Moir S A, Jones H. Mater Sci Eng, 1993; A173: 161 |
|
| No Suggested Reading articles found! |
|
|