| ELECTRON MICROSCOPY STUDY OF FIVE-FOLD TWINS IN ELECTRODEPOSITED NANO-TWIN Ni |
SHAN Haiquan1, ZHANG Yuefei1( ), MAO Shengcheng1, ZHANG Ze2 |
1 Institute of Microstructure and Properties of Advanced Materials, Beijing University of Technology, Beijing 100124 2 Department of Materials Science and Engineering, Zhejiang University, Hangzhou 310058 |
|
Cite this article:
SHAN Haiquan, ZHANG Yuefei, MAO Shengcheng, ZHANG Ze. ELECTRON MICROSCOPY STUDY OF FIVE-FOLD TWINS IN ELECTRODEPOSITED NANO-TWIN Ni. Acta Metall Sin, 2014, 50(3): 305-312.
|
|
|
Abstract The nanocrystalline Ni thin films with high density nano-scale growth twins were synthesized by direct electrodeposition technology. The five-fold twinning structure in electrodeposited nano-twin Ni was systematically investigated by TEM. The remarkable diffraction pattern and HRTEM images obtained from the cross-section observation demonstrate directly that the electrodeposited nano-twin Ni has five-fold twinning structure with five {111} twinned subcrystals and systematically analyzed the 7.35° intrinsic structural gap. In this work, the 7.35°gap was at least inset in two twin boundaries of the five-fold twin, the twin boundaries which share the 7.35° gap always broaden and was decomposed into other twins, so that, the grain present a irregular shape. cross-sectional TEM micrograph revealed that the electrodeposited nano-twin Ni had columnar grain structure with a strong {110} texture. By means of comprehensive structure characterization, a new space structural model of the five-fold twin was proposed.
|
|
Received: 25 July 2013
|
|
|
| Fund: Supported by National Natural Science Foundation of China (Nos.11374027 and 51001003) and Key Project Funding Scheme of Beijing Municipal Education Committee (No.KZ201010005002) |
| [1] |
Hermann C. Z Kristallogr, 1931; 79: 186
|
| [2] |
Segall R L. J Met, 1957; 9: 50
|
| [3] |
Melmed A J, Hayward D O. J Chem Phys, 1959; 31: 545
|
| [4] |
Zhu Y T, Liao X Z, Valiev R Z. Appl Phys Lett, 2005; 86: 103112
|
| [5] |
Zhu Y T, Liao X Z, Wu X L. Prog Mater Sci, 2012; 57: 1
|
| [6] |
Cao A J, Wei Y G. Appl Phys Lett, 2006; 89: 041919
|
| [7] |
Shao Y F, Wang S Q. Scr Mater, 2010; 62: 419
|
| [8] |
Huang P, Dai G Q, Wang F, Xu K W, Li Y H. Appl Phys Lett, 2009; 95: 203101
|
| [9] |
Bringa E M, Farkas D, Caro A, Wang Y M, McNaney J, Smith R. Scr Mater, 2008; 59: 1267
|
| [10] |
Lucadamo G, Medlin D L, Yang N Y C, Kelly J J, Talin A A. Philos Mag, 2005; 85: 2549
|
| [11] |
Sun Y G, Ren Y, Liu Y Z, Wen J G, Okasinski J S, Miller D J. Nat Commun, 2012; 3: 971
|
| [12] |
Narayan J, Srivatsa A R, Ravi K V. Appl Phys Lett, 1989; 54: 1659
|
| [13] |
An X H, Lin Q Y, Wu S D, Zhang Z F, Figueiredo R B, Gao N, Langdon T G. Scr Mater, 2011; 64: 249
|
| [14] |
Xia Y N, Xiong Y J, Lim B, Skrabalak S E. Angew Chem Int Ed, 2009; 48: 60
|
| [15] |
Marks L D. Rep Prog Phys, 1994; 57: 603
|
| [16] |
Hofmeister H. Cryst Res Technol, 1998; 33: 1
|
| [17] |
Hofmeister H. Encyclopedia Nanosci Nanotechnol, 2003; 3: 431
|
| [18] |
Li Q, Shao M W, Zhang S Y, Liu X M, Li G P, Jiang K, Qian Y T. J Crystal Growth, 2002; 243: 327
|
| [19] |
Fu X, Jiang J, Zhang W Z, Yuan J. Appl Phys Lett, 2008; 93: 043101
|
| [20] |
Chen H Y, Li J Q, Gao Y, Xie S S. Chin Electro Microsc Soc,2005; 24: 1
|
| [21] |
Cheng Y H, Zhang Y F, Mao S C, Han X D, Zhang Z. Acta Metall Sin, 2012; 48: 1342
|
|
(成宇浩, 张跃飞, 毛圣成, 韩晓东, 张 泽. 金属学报, 2012; 48: 1342)
|
| [22] |
Lu L, Chen X, Huang X, Lu K. Science, 2009; 323: 607
|
| [23] |
Lu L, Shen Y F, Chen X H, Qian L H, Lu K. Science, 2004; 304: 422
|
| [24] |
Hsiao H Y, Liu C M, Lin H W, Liu T C, Lu C L, Huang Y S, Chen C, Tu K N. Science, 2012; 336: 1007
|
| [25] |
Qu S X, Wang G M, Zhou H F, Huang Z L. Comput Mater Sci, 2011; 50: 1567
|
| [26] |
Chen M W, Ma E, Hemker K J, Sheng H W, Wang Y M, Cheng X M. Science, 2003; 300: 1275
|
| [27] |
Zhou G D,Guo K X. Electron Diffraction of Crystals and Quasicrystals. Beijing: Beijing University Press,1999: 222
|
|
(周公度,郭可信. 晶体和准晶体的衍射. 北京: 北京大学出版, 1999: 222)
|
| [28] |
Ino S, Ogawa S. J Phys Soc Jpn, 1967; 22: 1365
|
| [29] |
Li N, Wang J, Zhang X, Misra A. JOM, 2011; 63(9): 62
|
| [30] |
Gryaznov V G, Kaprelov A M, Heydenreich J. Cryst Res Technol, 1999; 34: 1901
|
| [31] |
Amblard J, Epelboin I, Froment M, Maurin G. J Appl Electrochem, 1979; 9: 233
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|