| MICROSTRUCTURE AND PHASE TRANSFORMATION OF Ni43Co7Mn41Sn9 HIGH TEMPERATURE SHAPE MEMORY ALLOY RIBBON |
| CHEN Feng1), SU Dexi1), TONG Yunxiang1), NIU Liqun1),WANG Haibo2), LI Li1) |
1) Center for Biomedical Materials and Engineering, Harbin Engineering University, Harbin 150001
2) College of Physics and Electronic Engineering, Taizhou University, Taizhou 318000 |
|
Cite this article:
CHEN Feng, SU Dexi, TONG Yunxiang, NIU Liqun,WANG Haibo, LI Li. MICROSTRUCTURE AND PHASE TRANSFORMATION OF Ni43Co7Mn41Sn9 HIGH TEMPERATURE SHAPE MEMORY ALLOY RIBBON. Acta Metall Sin, 2013, 49(8): 976-980.
|
|
|
Abstract NiCoMnSn shape memory alloy (SMA) is expected to be a promising high temperature SMA. However, the brittleness has become a big obstacle for its practical application. It is known that, grain refining is effective in improving the ductility of a specific metallic alloy. The aim of this work is to investigate the effect of melt--spinning on grain refinement and martensitic transformation and provide a guideline for the development of NiCoMnSn SMA. Ni43Co7Mn41Sn9 high temperature SMA ribbon was prepared by a single-roll melt-spinning method. The microstructure and martensitic transformation were investigated by means of OM, SEM, TEM, XRD and DSC, respectively. The experimental results showed that, the ribbon had a chemical composition close to the master alloy and exhibited a thermoelastic martensitic transformation at about 160℃. The grains in the as-spun ribbon, ranging from 2 μm to 18 μm,were remarkably refined compared with the master alloy. In the as--prepared ribbon,most of the columnar grains grew along the direction vertical to the ribbon plane.At room temperature, non-modulated martensite (tetragonal structure) consisting of twin substructure is determined in the ribbon after relieving the internal stress. Transformation temperatures were lowered by 30℃ after heat treatment at 400℃ for 1 h and then kept nearly constant with the increase of heat treatment temperatures.
|
|
Received: 02 April 2013
|
| [1] Kainuma R, Imano Y, Ito W, Morito H, Sutou Y, Oikawa K, Fujita A,Ishida K, Okamoto S, Kitakami O, Kanomata T. Appl Phys Lett, 2006; 88: 192513
[2] Han Z D, Wang D H, Qian B, Feng J F, Jiang X F, Du Y W. Jpn J Appl Phys, 2010; 49: 010211
[3] Krenke T, Duman E, Acet M, Moya X, Mannosa L, Planes A. J Appl Phys, 2007; 102: 033903
[4] Liu H S, Zhang C L, Han Z D, Xuan H C, Wang D H, Du Y W. J Alloys Compd, 2009; 467: 27
[5] Srivastava V, Chen X, James R D. Appl Phys Lett, 2010; 97: 014101
[6] Santamarta R, Cesari E, Pons J, Goryczka T. Metall Mater Trans, 2004; 35A: 761
[7] Shelyakov A V, Sitnikov N N, Koledov V V, Kuchin D S, Irzhak A I,Tabachkova N Y. Int J Smart Nano Mater, 2011; 2: 68
[8] Tong Y X, Chen F, Wang B L, Li L, Zheng Y F. Rare Met Mater Eng, 2010; 39: 2262
(佟运祥, 陈枫, 王本力, 李莉, 郑玉峰. 稀有金属材料与工程, 2010; 39: 2262)
[9] Chernenko V A, Kokorin V V, Vitenko I N. Smart Mater Struct, 1994; 3: 80
[10] Feng Y, Sui J H, Chen L, Cai W. Mater Lett, 2009; 63: 965
[11] Miyazaki S, Ishida A. Mater Sci Eng, 1999; A273-275: 106
[12] Ghodssi R, Lin P. MEMS Materials and Processes Handbook. New York: Springer, 2011: 361
[13] Zou M, Liu M Z, Dai S H, Xu M, Zhang F J, Gao Z M, Xie M M. Acta Metall Sin, 2001; 37: 691
(邹岷, 刘民治, 戴受惠, 徐民, 张凤军, 高忠民, 谢蒙萌. 金属学报, 2001; 37: 691)
[14] Chen F, Tong Y X, Huang Y J, Tian B, Li L, Zheng Y F. Intermetallics, 2013; 36: 81
[15] Otsuka K, Ren X. Progress Mater Sci, 2005; 50: 511
[16] He Z R, Zhou J E, Shuichi M. Acta Metall Sin, 2003; 39: 617
(贺志荣, 周敬恩, 宫崎修一. 金属学报, 2003; 39: 617)
[17] Rama Rao N V, Gopalan R, Manivel Raja M, Arout Chelvane J, Majumdar B, Chandrasekaran V. Scr Mater, 2007; 56: 405
[18] Santos J D, Sanchez T, Alvarez P, Sanchez M L, Sanchez Llamazares J L,Hernando B, Escoda L I, Sunol J J, Varga R. J Appl Phys, 2008; 103: 07B326
[19] Cai W, Feng Y, Sui J H, Gao Z Y, Dong G F. Scr Mater, 2008; 58: 830
[20] Pons J, Chernenko V A, Santamarta R, Cesari E. Acta Mater, 2000; 48: 3027
[21] Jiang C B, Muhammad Y, Deng L F, Wu W, Xu H B. Acta Mater, 2004; 52: 2779
[22] Segui C, Chernenko V A, Pons J, Cesari E, Khovailo V, Takagi T. Acta Mater, 2005; 53: 111
[23] Sozinov A, Likhachev A A, Lanska N, Ullakko K. Appl Phys Lett, 2002; 80: 1746
[24] Heczko O, Svec P, Janickovic D, Ullakko K. IEEE Trans Magn, 2002; 38: 2841
[25] Wu S K, Yang S T. Mater Lett, 2003; 57: 4291
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|