Acta Metall Sin  2013, Vol. 49 Issue (5): 530-536    DOI: 10.3724/SP.J.1037.2013.00007
Current Issue | Archive | Adv Search |
MOLECULAR DYNAMICS STUDY ON TEMPERATURE EFFECT AND RADIATION-DEDUCED DEFECT FORMATION IN hcp-Ti
YAO Man1), GAO Xiao1), ZENG Weipeng1), WANG Xudong1), XU Haixuan2), Simon R. Phillpot3)
1) School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024
2) Materials Science and Technology Division, Oak Ridge National Lab, Oak Ridge, TN 37831, USA
3) Department of Materials Science and Engineering, University of Florida, Gainesville, FL 32611, USA
Cite this article: 

YAO Man, GAO Xiao, ZENG Weipeng, WANG Xudong, XU Haixuan, Simon R. Phillpot. MOLECULAR DYNAMICS STUDY ON TEMPERATURE EFFECT AND RADIATION-DEDUCED DEFECT FORMATION IN hcp-Ti. Acta Metall Sin, 2013, 49(5): 530-536.

Download:  PDF(1858KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The radiation-induced defects formed in nuclear structure materials in the initial stage of displacement cascade and the subsequent changes in their microstructures and mechanical properties are the primary causes of their failure. Unfortunately the formation and aggregation of point defects are hard to be found only by probed experiments. In this work, the displacement cascade occurring in hcp-Ti system has been investigated by using molecular dynamics. After building the atomic model, by setting different PKA (primary knock-on atom) directions and PKA energies respectively, the evolution of simulated radiation-induced point defects in displacement cascade was studied and its two major characteristics, displacement and thermal spikes, have been given. The transient temperature distribution, local “melting region” variation in the damage zone caused by radiation as well as the peak and surviving numbers of Frenkel pairs were quantitatively estimated. For hcp-Ti, in the PKA energy region of 0.5-9.0 keV, the effect of PKA velocity direction on survival defect number is very small. Both the defect number at stable state and its maximum value have approximately linear relationship with the PKA energy.In the radiation evolution stage, the defects about 95 percent have recovered, the defect and temperature distribution caused by displacement cascade are asymmetric. The simulation method used in this paper would provide an effective way for the study on the evolution and micromechanism of radiation-induced point defects in displacement cascade.

Key words:  hcp-Ti      displacement cascade      molecular dynamics      radiation-induced defect      temperature     
Received:  05 January 2013     

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2013.00007     OR     https://www.ams.org.cn/EN/Y2013/V49/I5/530

[1] Wirth B D.  Science, 2007; 318: 92


[2] Matsukawa Y, Zinkle S J.  Science, 2007; 318: 959

[3] Tomas D R, Zbib H M, Khraishi T A, Wirth B D, Victoria M, Caturla M J.  Nature, 2000; 406: 871

[4] Odette G R, Alinger M J, Wirth B D.  Annu Rev Mater Res, 2008; 38: 471

[5] Sickafus K E, Grimes R W, Valdez J A, Cleave A, Tang M, Iahimaru M, Corish S, Stanek C R, Uberuaga B P.Nat Mater, 2007; 6: 217

[6] He X F, Yang W, Fan S.  Acta Phy Sin, 2009; 58: 8657

(贺新福, 杨文, 樊胜. 物理学报, 2009; 58: 8657)

[7] Domain C, Becquart C S.  Phys Rev, 2001; 65B: 02410

[8] Gameza L, Martinez E, Perlado J M, Cepas P, Caturla M J, Victoria M, Marian J, Arevalo C, Hernandez M, Gomez D.Fusion Eng Des, 2007; 82: 2666

[9] Bai X M, Voter A F, Hoagland R G, Nastasi M, Uberuaga B P.  Science, 2010; 327: 1631

[10] He B, Xue J M, Zou X Q, Wang Y G.  Acta Sci Nat Univ Pekin, 2009; 45: 385

(何斌, 薛建明, 邹雪晴, 王宇钢. 北京大学学报, 2009; 45: 385)

[11] Jin Z M, Chen Y X, Han J R, Lu D G.  Atomic Energy Sci Technol, 2009; 43: 501

(靳忠敏, 陈义学, 韩静茹, 陆道纲. 原子能科学技术, 2009; 43: 501)

[12] Bacon D J, Osetsky Y N, Stoller R, Voskoboinikov R E.  J Nucl Mater, 2003; 323: 152

[13] Xu H X.  From Electronic Structure of Point Defects to Physical Properties of Complex Materials Using Atomic-level Simulations. Gainesville: University of Florida, 2010: 148

[14] Wooding S J, Bacon J.  Philos Mag, 1995; 72A: 1261

[15] Liu J Z.  Nuclear Structural Materials. Beijing: Chemical Industry Press, 2007: 19

(刘建章. 核结构材料. 北京: 化学工业出版社, 2007: 19)

[16] Kim Y M, Lee B J, Baskes M I.  Phys Rev, 2006; 74B: 014101

[17] Baskes M I, Johnson R A.  Modelling Simul Mater Sci Eng, 1994; 2: 147

[18] Min S Y, KimY, Lee T K, Seo S, Jung H S, Kim D, Lee J, Lee B J.  Mater Int, 2010; 16: 421

[19] Biersack J P, Ziegler J F.  Nucl Instrum Methods Phys Res, 1982; 194: 93

[20] Yu J N.  Materials Radiation Effect. Beijing: Chemical Industry Press, 2007: 127

(郁金南. 材料辐照效应. 北京: 化学工业出版社, 2007: 127)

[21] Tsuchihira H, Oda T, Tanaka S.  J Nucl Mater, 2011; 414: 44

[22] Gao F, Bacon D J, Howe L M, So C B.  J Nucl Mater, 2001; 294: 288

[23] Norgett M J, Robinson M T, Torrens I M.  Nucl Eng Des, 1975; 33: 50

[24] Samaras M, Derlet P M, Swygenhoven H V, Victoria M.  Phys Rev Lett, 2002; 88: 12

[25] Psakhie S G, Zolnikov K P, Kryzhevich D S, Zheleznyakov A V, Chernov V M.  Phys Mesomech, 2009; 12: 20
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[3] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[4] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[5] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[6] CHENG Yuanyao, ZHAO Gang, XU Deming, MAO Xinping, LI Guangqiang. Effect of Austenitizing Temperature on Microstructures and Mechanical Properties of Si-Mn Hot-Rolled Plate After Quenching and Partitioning Treatment[J]. 金属学报, 2023, 59(3): 413-423.
[7] WANG Di, HE Lili, WANG Dong, WANG Li, ZHANG Siqian, DONG Jiasheng, CHEN Lijia, ZHANG Jian. Influence of Pt-Al Coating on Tensile Properties of DD413 Alloy at High Temperatures[J]. 金属学报, 2023, 59(3): 424-434.
[8] SHEN Zhao, WANG Zhipeng, HU Bo, LI Dejiang, ZENG Xiaoqin, DING Wenjiang. Research Progress on the Mechanisms Controlling High-Temperature Oxidation Resistance of Mg Alloys[J]. 金属学报, 2023, 59(3): 371-386.
[9] MIAO Junwei, WANG Mingliang, ZHANG Aijun, LU Yiping, WANG Tongmin, LI Tingju. Tribological Properties and Wear Mechanism of AlCr1.3TiNi2 Eutectic High-Entropy Alloy at Elevated Temperature[J]. 金属学报, 2023, 59(2): 267-276.
[10] WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei. Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K[J]. 金属学报, 2023, 59(2): 277-288.
[11] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[12] CHEN Jilin, FENG Guanghong, MA Honglei, YANG Dong, LIU Wei. Microstructure, Mechanical Properties, and Strengthening Mechanism of Cr-Mo Microalloy Cold Heading Steel[J]. 金属学报, 2022, 58(9): 1189-1198.
[13] XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui. Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. 金属学报, 2022, 58(8): 992-1002.
[14] CONG Hongda, WANG Jinlong, WANG Cheng, NING Shen, GAO Ruoheng, DU Yao, CHEN Minghui, ZHU Shenglong, WANG Fuhui. A New Design Inorganic Silicate Composite Coating and Its Oxidation Behavior at High Temperature in Steam Atmosphere[J]. 金属学报, 2022, 58(8): 1083-1092.
[15] LI Haiyong, LI Saiyi. Effect of Temperature on Migration Behavior of <111> Symmetric Tilt Grain Boundaries in Pure Aluminum Based on Molecular Dynamics Simulations[J]. 金属学报, 2022, 58(2): 250-256.
No Suggested Reading articles found!