| PHASE CONSTITUTION AND MORPHOLOGIES OF Mg-Zn-Zr ALLOY (MB15) |
| ZHANG Shaoqing Institute of Aeronautical Materials; Beijing ZHANG Shaoqing; Institute of Aeronautical Materlols. P. O. Box No.81; 100095 Beijing |
|
Cite this article:
ZHANG Shaoqing Institute of Aeronautical Materials; Beijing ZHANG Shaoqing; Institute of Aeronautical Materlols. P. O. Box No.81; 100095 Beijing. PHASE CONSTITUTION AND MORPHOLOGIES OF Mg-Zn-Zr ALLOY (MB15). Acta Metall Sin, 1989, 25(5): 36-41.
|
|
|
Abstract The equal-width lath-shaped Zn_2Zr_3 phase and the irregular lumpMgZn_2 phase were observed in the Zr- and Zn-enriched nucleus region and along thegrain boundaries of the as-cast alloy. The very fine ZnZr_2 phase occurs in thegrains and the supsr fine MgZn phase disperses in the α-Mg solid solution. In extrudedshapes, the coarse grains of Zn_2Zr_3 Phase and a great many dispersedly distributedZrH_2 phase and MgZn_2 phase particles appear in the Zr- and Zn-enriched lathregion. They are played an important role in impeding the proceeding of recrystal-lization. The precipitation of Mg_2Zn_3 Phase may be led to the non-lath region byageing at 170℃ for 10h.
|
|
Received: 18 May 1989
|
1 Emley E F. Principles of Magnesium Technology, London: Pergamon, 1966: 979 2 Bhambri AK, Kattamis T Z. AD 734770, 1971 3 #12 4 #12 5 Sturkey L. TMS AIME, 1960: 218: 466 6 Koster W, Muller F. Z Metallk, 1948; 39: 352 7 Clark J B. Acta Metall, 1965; 13: 1281 8 高桥恒夫,小岛阳,鹰西清.轻金属,1973;23:376 |
| No Suggested Reading articles found! |
|
|