Abstract The SiC_w/6061Al composite prepared by squeeze casting has a combi-nation of superior room temperature specific strength and modulus together with ex-cellent thermal properties. The extrusion can make an improvement on the strengthand ductility of the composite from 582 MPa as squeeze casted up to 639 MPa, andon the transformation from isotropic to the anisotropic structure. This seems to beexplained by the orientation of whiskers and the densification of dislocations inmatrix. TEM observation indicates that the stacking fault is the usual planar defecton the SiC_w surface.
1 Divecha A P, Fishman S G, Karmarkar S D. J Met, 1981; 33(9) : 12 2 Lederich R J, Sastry S M L. Mater Sci Eng, 1982; 55: 143 3 Nieh T G, Karlak R F. J Mater Sci Lett, 1983; 2: 119 4 Rack H J, Niskanen P W. Light Met Age, 1984; 42: 9 5 Cao L, Yao C K. Composites, to be published 6 Vogelsang M, Arsenault R J, Fisher R M. Metall Trans, 1986; 17A: 379 7 曹利.哈尔滨工业大学博士论文,1988