NUCLEATION AND GROWTH OF FERROUS MARTENSITES
ZHANG Xiumu;LI Yiyi Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

ZHANG Xiumu;LI Yiyi Institute of Metal Research; Academia Sinica; Shenyang. NUCLEATION AND GROWTH OF FERROUS MARTENSITES. Acta Metall Sin, 1991, 27(3): 19-26.

Download:  PDF(2729KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In situ observations of the nucleation and growth of ferrous marten-sites, including ε-, lenticular, butterfly, thin-plate and composite-plate ones at lowtemperature stage on optical or transmission electron microscope were carried out.The results confirmed the faulting model for the formation of ε-martensite proposedby Olson and Cohen. The grain boundaries and triple points are the favourable nu-cleation sites for the thin plates, and their surface relief grown initially like asmall needle. The lenticular martensite was observed as two stages of formation.According to the dislocation resolving reaction:a/6[111]_b→a/3[111]_b+a/2[111]_b, the emission dislocation(b=a/2[111]_b) acting as thedislocation soulce for the transition of lattice invariant shear from twinning to slipwas proposed.
Key words:  martensite      nucleation      growth      observation      emission dislocation     
Received:  18 March 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I3/19

1 Olson G B, Cohen M. Metall Trans, 1976; 7A: 1897--1915
2 蒋生蕊,金属学报,1986;22:A393;1988;24(增刊Ⅰ):A 40
3 Zhang X M, Gautier E, Simon A. Acta Metall, 1989; 37: 487
4 Kajiwara S. Metall Trans, 1986; 17A: 1693
5 Schumann H. Prakt Metallogr, 1975; 12: 511
6 Shimizu K, Tanaki T. Trans Jpn Inst Met, 1978; 19: 685
7 Brooks J W, Lorotto M H, Smallmann R E. Acta Metall, 1979; 27: 1839
8 Zhang Xiumu, Li Yiyi, Chen Lang, Li Hengwu. ICOMAT-86, Nara, Japan, 1986, Japan Inst Metals, 1987: 482
9 Sleeswyk A W. Acta Metall, 1962; 10: 705
10 Kakesnita T, Shimizu K, Maki T, Tamura I. Scr Metall, 1980; 14: 1067
11 Sadovsky V D. Proc ICOMAT-86, Nara. Japan, 1986, Japan Inst Metals, 1987. 222
12 Okamoto H, Oka M. Proc ICOMAT-86, Nara, Japan, 1986, Japan Inst Metals, 1987: 276
13 Zhang X M, Zhao X, Zhong J X, Qi Y. Scr Metall, 1990; 24: 1594
14 Wen Youhai, Zhang Xiumu, Zhao Xu, Li Yongsen. Chin J Met Sci Technol, 1991; 7(3) : 211
15 Zhao X, Zhang X M, He Y Y, Li B. Cryogenics, 1990; 30: 404
16 Gong H, Zhang X M. Mater Forum, 1990; 14: 137--141
17 贡海,章为夷,张修睦.金属学报,1991;27(3) :A201
[1] WANG Zhoutou, YUAN Qing, ZHANG Qingxiao, LIU Sheng, XU Guang. Microstructure and Mechanical Properties of a Cold Rolled Gradient Medium-Carbon Martensitic Steel[J]. 金属学报, 2023, 59(6): 821-828.
[2] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[3] CHEN Xueshuang, HUANG Xingmin, LIU Junjie, LV Chao, ZHANG Juan. Microstructure Regulation and Strengthening Mechanisms of a Hot-Rolled & Intercritical Annealed Medium-Mn Steel Containing Mn-Segregation Band[J]. 金属学报, 2023, 59(11): 1448-1456.
[4] HOU Xuru, ZHAO Lin, REN Shubin, PENG Yun, MA Chengyong, TIAN Zhiling. Effect of Heat Input on Microstructure and Mechanical Properties of Marine High Strength Steel Fabricated by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(10): 1311-1323.
[5] QI Zhao, WANG Bin, ZHANG Peng, LIU Rui, ZHANG Zhenjun, ZHANG Zhefeng. Effects of Stress Ratio on the Fatigue Crack Growth Rate Under Steady State of Selective Laser Melted TC4 Alloy with Defects[J]. 金属学报, 2023, 59(10): 1411-1418.
[6] LI Xiaolin, LIU Linxi, LI Yating, YANG Jiawei, DENG Xiangtao, WANG Haifeng. Mechanical Properties and Creep Behavior of MX-Type Precipitates Strengthened Heat Resistant Martensite Steel[J]. 金属学报, 2022, 58(9): 1199-1207.
[7] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[8] LI Xifeng, LI Tianle, AN Dayong, WU Huiping, CHEN Jieshi, CHEN Jun. Research Progress of Titanium Alloys and Their Diffusion Bonding Fatigue Characteristics[J]. 金属学报, 2022, 58(4): 473-485.
[9] TIAN Zhihua, ZHANG Peigen, LIU Yushuang, LU Chengjie, DING Jianxiang, SUN Zhengming. Research Progress and Outlook of Metal Whisker Spontaneous Growth on MAX Phase Substrates[J]. 金属学报, 2022, 58(3): 295-310.
[10] ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng. Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation[J]. 金属学报, 2022, 58(2): 155-164.
[11] ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue. Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels[J]. 金属学报, 2022, 58(2): 193-205.
[12] HAN Ruyang, YANG Gengwei, SUN Xinjun, ZHAO Gang, LIANG Xiaokai, ZHU Xiaoxiang. Austenite Grain Growth Behavior of Vanadium Microalloying Medium Manganese Martensitic Wear-Resistant Steel[J]. 金属学报, 2022, 58(12): 1589-1599.
[13] SHI Zengmin, LIANG Jingyu, LI Jian, WANG Maoqiu, FANG Zifan. In Situ Analysis of Plastic Deformation of Lath Martensite During Tensile Process[J]. 金属学报, 2021, 57(5): 595-604.
[14] WANG Yu, HU Bin, LIU Xingyi, ZHANG Hao, ZHANG Haoyun, GUAN Zhiqiang, LUO Haiwen. Influence of Annealing Temperature on Both Mechanical and Damping Properties of Nb-Alloyed High Mn Steel[J]. 金属学报, 2021, 57(12): 1588-1594.
[15] XU Junfeng, ZHANG Baodong, Peter K Galenko. Model of Eutectic Transformation Involving Intermetallic Compound[J]. 金属学报, 2021, 57(10): 1320-1332.
No Suggested Reading articles found!