| THERMODYNAMICS OF MARTENSITIC TRANSPORMATION IN β-Cu BASE ALLOYS |
| XU Zuyao T. Y. Hsu; ZHOU Xiaowang Shanghai Jiaotong University |
|
Cite this article:
XU Zuyao T. Y. Hsu; ZHOU Xiaowang Shanghai Jiaotong University. THERMODYNAMICS OF MARTENSITIC TRANSPORMATION IN β-Cu BASE ALLOYS. Acta Metall Sin, 1991, 27(3): 13-18.
|
|
|
Abstract An approach for the thermodynamics of the thermoelastic martensitictransformation in β-Cu base alloys is suggested. Driving forces for martensitic trans-formation, T_0 and M_s temperatures in Cu-Zn, Cu-Al and Cu-Zn-Al alloys werecalculated and the calculated M_s are in good agreement with the experimental ones.Ordering of the parent phase lowers M_s in Cu-Zn and Cu-Zn-Al alloys, but risesM_s (T_0) in Cu-Al alloys. Two methods for estimation of the non-chemical freeenergy attending the thermoelastic martensitic transformation are also introduced.
|
|
Received: 18 March 1991
|
1 Tong H G, Wayman C M. Acta Metall, 1975: 23: 209 2 Humbeeck J V, Janssen J, Mwamba-Ngoie, Delaey L. Scr Metall, 1984; 18: 893 3 Selected Values of the Thermodynamic Properties of Binary Alloys, Metals Park, Ohio: ASM, 1973: 812, 151 4 Inden G. Z Metallk, 1975; 66: 648 5 Cornelis I, Wayman C M. Acta Metall, 1974; 22: 291 6 Zhou X W, Hsu T Y (Xu Zuyao). Acta Metall, 1989; 37: 3085 7 Warlimont H, Delaey L, Krishnan R V, Has T. J Mater Sci, 1974; 9: 1545 8 Pops H, Massalski T B. Trans Metall Soc AIME, 1964; 230: 1662 9 Rapacioli R, Ahlers M. Scr Metall, 1977; 11: 1147 10 Singh S C, Murakami Y, Delaey L. Scr Metall. 1978; 12: 435 11 Ahlers M. Prog Mater Sci, 1986; 30 12 Abu-Arab A, Ahlers M. Acta Metall, 1988; 36: 2627 13 Swan P R, Warlimont H. Acta Metall, 1963; 11: 511 14 Hsu T Y (Xu Zuyao), Zhou X W, Humbeeck J V, Delaey L. Scr Metall, Mater, 1991; 25:165 16 刘锦文,李俊惠,隋晓红,顾敏,阳志英,中南矿冶学院学报,1983;38;43 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|