Mechanical Properties and Creep Behavior of MX-Type Precipitates Strengthened Heat Resistant Martensite Steel
LI Xiaolin1(), LIU Linxi1, LI Yating1, YANG Jiawei1, DENG Xiangtao2, WANG Haifeng1
1.State Key Laboratory of Solidification Processing & Center of Advanced Lubrication and Seal Materials, Northwestern Polytechnical University, Xi'an 710072, China 2.State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China
Cite this article:
LI Xiaolin, LIU Linxi, LI Yating, YANG Jiawei, DENG Xiangtao, WANG Haifeng. Mechanical Properties and Creep Behavior of MX-Type Precipitates Strengthened Heat Resistant Martensite Steel. Acta Metall Sin, 2022, 58(9): 1199-1207.
There has been a push in the past few decades to increase the operating temperature of steam generators to the ultra-supercritical (USC) regime. This requires that creep-resistant alloys can operate at 650-700°C for 30 years. P91 and P92 steels are commercially applied in USC steam generator applications. However, these steels fail due to the coarsening of M23C6 and Laves phases during long-term service. Therefore, it is significant to restrict the formation of easily coarsened precipitates. In this study, a martensitic heat-resistant steel strengthened by single MX precipitates is designed using the Thermo-Calc software, as Fe-0.03C-10Cr-0.2Zr-0.3V. The yield strength, tensile strength, and elongation at room temperature are 266 MPa, 413 MPa, and 38%, respectively. The high-temperature hardnesses of specimens aged at 700oC for 1, 10, 100, and 1000 h were tested at 700oC after normalizing treatment, which illustrates that the high-temperature hardness of the specimens remains stable with increased aging time. In addition, TEM was used to characterize the precipitates in the heat-resistant steel aged for different times. It is found that with the increase of aging time (1-1000 h), the average size of the precipitates increases from 10.8 to 17.8 nm. The composition of MX precipitates in the specimens aged for 1000 h is Zr0.46Nb0.14C0.4 and the volume fraction is 0.29%. According to the creep test results, the threshold stresses at 650 and 700oC are 54.5 and 28.4 MPa, respectively.
Fig.1 Phase diagrams of P91 steel (0.1C-9Cr-1Mo-0.22V-0.08Nb-0.3Ni-0.05N-0.23Si-0.04Mn) (a) and T alloy (0.1C-9Cr-0.22V-0.08Nb-0.05Zr-0.12Ti-1.2W-0.12Ni-0.8Mn-0.15Si) (b)
Fig.2 Schematics for composition design and screening process (V—volume fraction of phase)
Fig.3 Phase diagram (a) and step diagram (b) of the designed heat-resistant steel
Fig.4 OM (a) and TEM (b) images of Fe-0.03C-10Cr-0.2Zr-0.3V steel by HR + N treatment and aged at 700oC for 1 h (HR + N—hot rolling + normalizing at 1000oC for 1 h)
Fig.5 Morphologies and size distributions of precipitates (Stdev—standard deviation) (a-f) TEM images (a-c) and size distributions (d-f) of precipitates formed in Fe-0.03C-10Cr-0.2Zr-0.3V steel aged at 700oC for 10 h (a, c), 100 h (b, e), and 1000 h (c, f) after HR + N treatment (g-i) SEM (g, h) and TEM (i) images of Fe-0.03C-10Cr-0.2Zr-0.3V steel aged at 700oC for 1000 h after HR treatment without corrosion (g) and after corrosion (h, i) (Arrows in Fig.5h point to the spherical precipitates)
Fig.6 Composition analyes of precipitates formed in Fe-0.03C-10Cr-0.2Zr-0.3V steel aged at 700oC for 1000 h after HR + N treatment by EDS analysis (a) and Thermo-Calc prediction (b)
Method
Atomic fraction
Mass fraction
Zr
Nb
C
Zr
Nb
C
TEM-EDS analysis
0.46
0.14
0.40
0.71
0.21
0.08
Thermo-Calc prediction
0.42
0.093
0.49
0.723
0.165
0.112
Table 1 Chemical composition of precipitates formed in Fe-0.03C-10Cr-0.2Zr-0.3V steel aged at 700oC for 1000 h after HR + N treatment
Fig.7 HRTEM image (a), and FFT (b) and IFFT (c) diagrams of precipitate formed in Fe-0.03C-10Cr-0.2Zr-0.3V steel aged at 700oC for 1000 h after HR + N treatment
Fig.8 High-temperature Vickers hardnesses of Fe-0.03C-10Cr-0.2Zr-0.3V steel tested at 700oC
Fig.9 Creep properties of Fe-0.03C-10Cr-0.2Zr-0.3V steel tested at 650oC (a, c) and 700oC (b, d) (σth—threshold stress) (a, b) minimum creep rate vs applied stress (c, d) (creep rate)1/4vs applied stress
1
Fedoseeva A, Dudova N, Kaibyshev R. Creep strength breakdown and microstructure evolution in a 3%Co modified P92 steel [J]. Mater. Sci. Eng., 2016, A654: 1
2
Tkachev E, Belyakov A, Kaibyshev R. Creep behavior and microstructural evolution of a 9%Cr steel with high B and low N contents [J]. Mater. Sci. Eng., 2018, A725: 228
3
Xu Y T, Li W, Wang M J, et al. Nano-sized MX carbonitrides contribute to the stability of mechanical properties of martensite ferritic steel in the later stages of long-term aging [J]. Acta Mater., 2019, 175: 148
doi: 10.1016/j.actamat.2019.06.012
4
Lee K H, Suh J Y, Hong S M, et al. Microstructural evolution and creep-rupture life estimation of high-Cr martensitic heat-resistant steels [J]. Mater. Charact., 2015, 106: 266
doi: 10.1016/j.matchar.2015.06.005
5
Abe F, Ohba T, Miyazaki H, et al. Effect of W-Mo balance and boron nitrides on creep rupture ductility of 9Cr steel [J]. Mater. High Temp., 2019, 36: 368
doi: 10.1080/09603409.2019.1574369
6
Abe F. Creep deformation behaviour and its effect on creep life and rupture ductility of W-Mo-balanced 9Cr steels [J]. Mater. High Temp., 2020, 37: 165
doi: 10.1080/09603409.2020.1735208
7
Yang K, Liang Y, Yan W, et al. Preferential distribution of boron and its effect on microstructure and mechanical properties of (9~12)%Cr martensitic heat resistant steels [J]. Acta Metall. Sin., 2020, 56: 53
Isik M I, Kostka A, Eggeler G. On the nucleation of Laves phase particles during high-temperature exposure and creep of tempered martensite ferritic steels [J]. Acta Mater., 2014, 81: 230
doi: 10.1016/j.actamat.2014.08.008
9
Isik M I, Kostka A, Yardley V A, et al. The nucleation of Mo-rich Laves phase particles adjacent to M23C6 micrograin boundary carbides in 12% Cr tempered martensite ferritic steels [J]. Acta Mater., 2015, 90: 94
doi: 10.1016/j.actamat.2015.01.027
10
Lu Q, Xu W, van der Zwaag S. The computational design of W and co-containing creep-resistant steels with barely coarsening laves phase and M23C6 as the strengthening precipitates [J]. Metall. Mater. Trans., 2014, 45A: 6067
11
Liu F, Rashidi M, Johansson L, et al. A new 12% chromium steel strengthened by Z-phase precipitates [J]. Scr. Mater., 2016, 113: 93
doi: 10.1016/j.scriptamat.2015.10.030
12
Rashidi M, Golpayegani A, Sheikh S, et al. Mechanistic insights into the transformation processes in Z-phase strengthened 12% Cr steels [J]. Mater. Des., 2018, 158: 237
doi: 10.1016/j.matdes.2018.08.006
13
Cipolla L, Danielsen H K, Venditti D, et al. Conversion of MX nitrides to Z-phase in a martensitic 12% Cr steel [J]. Acta Mater., 2010, 58: 669
doi: 10.1016/j.actamat.2009.09.045
14
Rashidi M, Johansson L, Andrén H O, et al. Microstructure and mechanical properties of two Z-phase strengthened 12%Cr martensitic steels: The effects of Cu and C [J]. Mater. Sci. Eng., 2017, A694: 57
15
Danielsen H K, Di Nunzio P E, Hald J. Kinetics of Z-Phase precipitation in 9 to 12 pct Cr steels [J]. Metall. Mater. Trans., 2013, 44A: 2445
16
Rashidi M, Odqvist J, Johansson L, et al. Experimental and theoretical investigation of precipitate coarsening rate in Z-phase strengthened steels [J]. Materialia, 2018, 4: 247
doi: 10.1016/j.mtla.2018.09.024
17
Liu Z, Liu Z D, Wang X T, et al. Evolution of the microstructure in aged G115 steels with the different concentration of tungsten [J]. Mater. Sci. Eng., 2018, A729: 161
18
Xiao B, Xu L Y, Tang Z X, et al. A physical-based yield strength model for the microstructural degradation of G115 steel during long-term creep [J]. Mater. Sci. Eng., 2019, A747: 161
19
Taneike M, Abe F, Sawada K. Creep-strengthening of steel at high temperatures using nano-sized carbonitride dispersions [J]. Nature, 2003, 424: 294
doi: 10.1038/nature01740
20
Zhao J F, Gong J D, Saboo A, et al. Dislocation-based modeling of long-term creep behaviors of Grade 91 steels [J]. Acta Mater., 2018, 149: 19
doi: 10.1016/j.actamat.2018.02.001
CHU Wuyang; LU Rongbang;QIAO Lijie; WANG Yanbin (Department of Materials Physics; University of Science & Technology Beijing; Beijing 100083)CHENG Yihuan; CHEN Hongxing(Baoshan Iron and Steel Corporation; Shanghai 201900);GUAN Yongsheng; YAN Yinglong; SUN Wei(Tianjin Steel Pipe Corporation; Tianjin 300310)Correspondent:CHU Wuyang; professor Tel: (010)62332906; Fax: (010)62327283;E-mail: ljqiao@public.bta.net.cn. THE THRESHOLD STRESS FOR HYDSOGEN-INDUCED CRACKING OF C90 TUBULAR STEELS[J]. 金属学报, 1998, 34(10): 1077-1083.