Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (3): 27-32    DOI:
Current Issue | Archive | Adv Search |
BUTTERFLY MARTENSITE NUCLEI IN AN Fe-Ni-V-C ALLOY
CHEN Qizhi;WU Xingfang;KE Jun T. Ko University of Science and Technology Beijing
Cite this article: 

CHEN Qizhi;WU Xingfang;KE Jun T. Ko University of Science and Technology Beijing. BUTTERFLY MARTENSITE NUCLEI IN AN Fe-Ni-V-C ALLOY. Acta Metall Sin, 1991, 27(3): 27-32.

Download:  PDF(2394KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The butterfly martensite nuclei in an Fe-Ni-V-C alloy were observedunder TEM to consist of the enveloping dislocations with Burgers vector 1/2[011]_(fcc)and the arrays of dislocations with Burgers vector 1/2[110]_(fcc) piled up within theformers. The enveloping dislocations and the arrays of dislocations provide the re-quired shear when the planes (111)_(fcc) move over each other to alter their stackingorder and change into the planes (110)_(bcc) respectively. The neccessary adjustment ofthe spacings is provided by the dislocations in martensite. The crystallographic rela-tionship after double-shear is K-S one.
Key words:  butterfly martensite      nuclei      enveloping dislocation      piling dislocation     
Received:  18 March 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I3/27

1 Kikuchi T, Kajimara S. In: Delaey L, Chandrasekaran M eds., Proc ICOMAT-1982, August, 8--12, 1982, Leuven, 1982: 109
2 Loretto M H, Butler E P. In: Fujita H ed., Proc Int Symposim on Behavier of Lattice Imperfections in Materials-In Situ Experiments with High Voltage Electron Microscopes (HVEM), Research Center for Ultra-High Voltage Electron Microscopy, Osaka, Japan, 1985: 85
3 Katayama T, Fujita H. In: Fujita H ed., Proc Int Symposim on Behavier of Lattice Imperfections in Materials-In Situ Experiments with High Voltage Electron Microscpoes (HVEM), Research Center for Ultra-High Voltage Electron Microscopy, Osaka, Japan, 1985: 103
4 张修睦,李依依.金属学报,1991;27:A179
5 Olson G B, Cohen M. Metall Trans, 1976; 7A: 1897
6 Foreman A J, Jaswon M A, Wood J K. Proc Phys Soc, 1951; A64: 156
7 Chen Qizhi, Wu Xing fang, Ke Jun. Acta Metall, to be published[
[1] JIAN Zengyun, LI Na, CHANG Fang'e, FANG Wen, ZHAO Zhiwei, DONG Guangzhi,JIE Wanqi. MOLECULAR DYNAMICS SIMULATION OF THE ATOM CLUSTER EVOLUTION IN COPPER MELT DURING SOLIDIFICATION PROCESS[J]. 金属学报, 2012, 48(6): 703-708.
[2] YANG Jiguang Tianjin UniversityWANG Chumpi.associare professor;Faculty of Foundry.Tianjin Unicersity .Tianjin 300072. GRAPHITE NUCLEI IN CAST IRON UNDER INOCULATION TREATMENT[J]. 金属学报, 1993, 29(5): 63-67.
[3] LIU Jinshui;SHU Zhen;LI Chuanping Hunan University; Changsha. INFLUENCE OF TI ON STRUCTURE AND PROPERTLES OF HIGH Al-Zn ALLOYS[J]. 金属学报, 1993, 29(11): 9-13.
[4] LU Ke Institute of Metal Research;Academia Sinica;Shenyang;WANG Jingtang Institute of Metal Research; Academia Sinica; Shenyang. RELATIONSHIP BETWEEN CRYSTALLIZATION TEMPERATURE AND PRE-EXISTING NUCLEI IN THE AMORPHOUS Ni-P ALLOY[J]. 金属学报, 1988, 24(2): 171-175.
No Suggested Reading articles found!