| OXIDATION OF RAPIDLY QUENCHED Au-Si RIBBON DURING PROLONGED ATMOSPHERIC CRYSTALLIZATION |
| LU Yicheng;WANG Jun;YANG Chunsheng;JIN Shunfa Shanghai Jiaotong University |
|
Cite this article:
LU Yicheng;WANG Jun;YANG Chunsheng;JIN Shunfa Shanghai Jiaotong University. OXIDATION OF RAPIDLY QUENCHED Au-Si RIBBON DURING PROLONGED ATMOSPHERIC CRYSTALLIZATION. Acta Metall Sin, 1993, 29(2): 74-77.
|
|
|
Abstract The rapidly quenched Au-17.9at. -%Si ribbon has become twisted, brittle,disappeared from eutectic point and started to melt up to 1341 K after prolongedcrystallization for 3 years under atmospheric environment. This seems to be due to theoxidation of Si in the eutectic of Au-Si into SiO_2.
|
|
Received: 18 February 1993
|
1 Okamoto H, Massalski T B. Bull Alloy Phase Diagr. 1983; 4: 190 2 Bhattacharya D, Johnson A A, Sorem R R, Anderson G A. Mater Sci Eng, 1978; 32: 181 3 Anderson G A, Bestel J L, Johnson A A, Post B. Mater Sci Eng, 1971; 7: 83 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|