PHASE DIAGRAMS OF SmCl_3-PbCl_2 AND SmCl_3-PbCl_2-CaCl_2
WANG Shulan;ZHANG Yifeng;SUI Dianpeng Northeast University of Technology; Shenyang
Cite this article:
WANG Shulan;ZHANG Yifeng;SUI Dianpeng Northeast University of Technology; Shenyang. PHASE DIAGRAMS OF SmCl_3-PbCl_2 AND SmCl_3-PbCl_2-CaCl_2. Acta Metall Sin, 1993, 29(2): 70-73.
Abstract Phase diagrams of binary system SmCl_3-PbCl_2 and ternary systemSmCl_3-PbCl_2-CaC_2, have been determined by DTA and X-ray diffraction analyses. In theSmCl_3-PbCl_2 system, an incongruent compound 3SmCl_3-PbCl_2, an eutectic point at 452℃containing 33.0 mol-% SmCl_3 and a peritectic point at 465℃ containing 42.0 mol-%SmCl_3 were obtained. In the SmCl_3-PbCl_2-CaCl_2 system, 4 liquiduses corresponding to theprimary crystallization of SmCl_3, PbCl_2, CaCl_2, and 3SmCl_3·PbCl_2, respectively, 5unvariant lines related to the secondary crystallization, a ternary eutectic point at 396℃ con-taining 29.5 SmCl_3 and 58.0 PbCl_2 by mol-% and a ternary peritectic point at 417℃ con-taining 36.0 SmCl_3 and 50.0 PbCl_2 by mol-% were found. Two reactions corresponding to 4phase equilibriums are L=CaCl_2+PbCl_2+3SmCl_3·PbCl_2 and L+SmCl_3=CaCl_2+3SmCl_3·PbCl_2.
1 张翊凤,孟波.金属学报,1991;27:B438 2#12 1970;43(8) :1835 3 Coleman D S, Long P D A. Trans Inst Min Metall, 1968; 77C: 170 4 苏勉曾,李根培.化学通报,1979;(4) :34 5 乔芝郁,王明生,郑朝贵,段淑贞.金属学报,1989;25:B234 6 郑朝贵,刘红平,乔芝郁,叶于浦.金属学报,1990;26:B68
YUAN Wenxia; MA Shulan; QIAO Hin; ZHUANG Weidong; XING Xianran;QIAO Zhiyu (University of Science and Technology Beijing; Beijing 100083)(General Institute for Non-Ferrous Metals; Beijing 100088)(Manuscript received 1995-04-28; in revised form 1995-11-05). A STUDY ON THE YCl_3-AECl_2(AE=Mg, Ca, Sr, Ba)BINARY PHASE DIAGRAMS[J]. 金属学报, 1996, 32(2): 139-143.
YAN Licheng;FANG Jianhui;XU Jingyan;YANG Jinxiu(Shanghai University of Science and Technology). PHASE DIAGRAM OF KF-LiCl-CaCl_2 SYSTEM[J]. 金属学报, 1994, 30(19): 301-303.
SHEN Jianyun(General Research Institute for Non-Ferrous Metals;Beijing);CHATILLON C(Laboratoire de Thermodynamique et Physico-chimie Metallurgiques;Fracne)(Manuscript received 16 June;1993). THERMODYNAMICS OF Ga-In-As SYSTEM UNDER LATTICE DEFORMATION[J]. 金属学报, 1994, 30(16): 145-149.